← Knowledge Center

The sealing step illustrates 30% thinner and a recoat check at about 2 hours. Confirm project-specific conditions before use. At about 19 seconds, 0.8–1 m²/kg is the N600 midcoat coverage shown in this demonstration. The N600 TDS (V2.7, page 4) gives a reference consumption of 0.6–1.0 kg/m² for the midcoat. Verify actual consumption, recoating conditions and readiness for traffic on the project substrate and site trial.

Gaodun Polyaspartic Flake Flooring Application Procedure

Updated synthetic narration and matching guide subtitles (8 November 2026). Original footage may contain older parameters; use the updated guide and current model-specific TDS.

English SRT · 繁體 SRT

Open the high-resolution original with its original soundtrack

VIDEO DESCRIPTION

Video Description

  1. Step 1: Prepare the substrate.

    Abrade the concrete and remove laitance, loose layers and oil. Repair cracks, level by abrasion and vacuum thoroughly to obtain a sound, clean and dry substrate. Treat expansion and moving joints separately.

  2. Step 2: Penetration sealing.

    This N600 concrete sealing example used compatible thinner at 30% of the mass of the undiluted A+B mix. Each kilogram of undiluted mix covered about 4 m². The example calls for checking readiness to recoat after about 2 hours. The N600 TDS (V2.7) specifies a 1:1 A:B mass ratio and gives a reference sealing coverage of about 3–4 m²/kg. Before work, obtain written thinning instructions from Gaodun for the project substrate. Apply the midcoat only after confirming recoating conditions for the actual temperature, humidity and coating condition.

  3. Step 3: Apply N600 and broadcast flakes to full coverage.

    Mix N600 at the specified ratio and squeegee or roll evenly. The recorded N600 midcoat application covered 0.8–1 m² per kg of mixed coating. N600 TDS V2.7, page 4, gives 0.6–1.0 kg/m² for the midcoat. Confirm actual consumption on a site trial. Broadcast flakes uniformly while wet for full coverage without exposed binder areas.

  4. Step 4: Recover loose flakes, trim and vacuum.

    After approximately 5–10 hours of cure, confirm the surface can support the work. Collect clean, dry, unbonded flakes, sieve and store sealed for reuse. Scrape across the surface to remove raised or poorly bonded flakes; lightly abrade if needed, then vacuum thoroughly.

  5. Step 5: Apply N200 clear finish.

    Mix Gaodun clear N200 at its specified ratio and squeegee or roll evenly. Indicative total consumption is 1 kg/m² to seal the flake layer and form a clear, hard, abrasion-resistant protective finish. Determine the number of coats from the permitted single-coat thickness and actual sealing results.

This video records an actual polyaspartic polyurea application procedure. Assess the application, substrate type and condition, product grade, A/B ratio, consumption, successive coats and curing conditions together.

APPLICATION INFORMATION

Application Information

Material system
Polyaspartic polyurea
Category
Application procedure
Models mentioned
N600, N200
Publisher
Shenzhen Gaodun New Materials Co., Ltd.
Purpose
Application procedure or case reference
Before application
Model-specific TDS, SDS, substrate and environmental conditions

Publisher: Shenzhen Gaodun New Materials Co., Ltd.
First published:

Content limits: Application videos and case records explain particular processes and project conditions. Before work, check the substrate, environment and details against the model-specific documents and a site trial.