Polyaspartic Polyurea Technical ArticlesWhat Are the Advantages of Polyaspartic Polyurea? Weatherability, Fast Curing and High Solids through Film Formation
Polyaspartic polyurea enables rapid film formation through a two-component reaction and provides design space for outdoor color retention and high solids formulations. Each of the three advantages has its own conditions. The outdoor weather resistance depends on the film formation raw materials on both sides and the finished product test. The construction efficiency depends on the operability time after mixing, overcoating and open conditions. The applicable volume solid content and target dry film thickness should be used to estimate the coating amount. This article takes clear topcoat as an example to explain how to distinguish between aliphatic and systems with aromatic structures, and how to use the technical data of the same finished product to check the weather resistance, curing and construction data required for selection. When selecting materials, you can also obtain the technical data sheet of the corresponding finished product from the supplier and check whether the construction conditions are consistent with the actual project.
Article contents (6 sections)
The polyaspartic polyurea mentioned in this article, the full name of polyaspartic polyurea, is usually formed by the reaction of polyaspartic ester resin containing secondary amine group and curing agent containing isocyanate group. The active hydrogen on the secondary amine participates in the reaction to form a urea bond. Raw materials with multiple reaction sites can connect molecules into cross-linked networks. Even if the solvent evaporates during construction, the formation of a solid film from the liquid material still relies on a two-component reaction. [1]
A published formulation study gives examples of raw materials on the resin side. The researchers performed Michael addition of isophorone diamine (IPDA) and diethyl maleate (DEM) to first prepare polyaspartic ester resin, and then added isocyanate curing agent to form a film. IPDA is a cycloaliphatic diamine, the molecule has a ring, and the nature of the ring is alicyclic. This example explains how cycloaliphatic diamine becomes the structural source of the resin. It also shows that after purchasing a two-component paint, the prepared resin components and curing agent are mixed on site. The research formula contains experimental solvents and specific additives, and its film formation results are limited to the paper samples. [1][2]
There are also identifiable sources of structure on the hardener side. BASF's technical sheet for Basonat® HI 100 NG MB describes the product as an isocyanurate-type polyisocyanate based on hexamethylene diisocyanate (HDI). It shows that aliphatic isocyanate can be made into a multifunctional curing agent. The application given in this information is two-component polyurethane and is only used to identify the structure of raw materials. When switching to the polyaspartic polyurea formula, it is still necessary to check the two sets of distribution ratios, construction performance and film formation results. [3]
Construction personnel should mix ingredients according to the mass ratio or volume ratio specified in the finished product technical data sheet (TDS). The production formula is based on the amount of effective reactive groups on both sides. The on-site ratio also includes the mass or volume of pigments, fillers and other components in each barrel. Treating the mass ratio as a volume ratio, or adding more curing agent to accelerate drying, will change the original reaction ratio. When there are sticky, soft, hard and brittle or local curing inconsistencies, the first step should be to check the ingredients and mixing records.
Why aliphatic polyaspartic polyurea is suitable for prioritizing outdoor color retention
For outdoor surfaces that require color retention, the main film formation reaction raw materials on both sides are polyaspartic polyurea with aliphatic or cycloaliphatic structures, which is a formula direction worthy of priority verification. The Covestro manual uses a combination of polyaspartic ester and aliphatic polyisocyanate to develop weather-resistant coatings. The American Chemistry Council's Technical Note on Building Coatings also lists UV resistance and color retention as reasons for selecting aliphatic diisocyanate systems. Surface layers containing aromatic isocyanate structures have a higher risk of visible yellowing under light. The actual differences must still be compared under the same color, film thickness, substrate, compatible system and exposure procedures. [1][6]
An original study examined light exposure on transparent aromatic polyurethane coatings on glass panels. The coating is prepared from castor oil and diphenylmethane diisocyanate (MDI), and research focuses on photooxidation and yellowing. This study can be used as circumstantial evidence to identify the appearance risks of aromatic isocyanate coating. Its polyurethane formula is different from polyaspartic polyurea, and it cannot be used to quantify the weather resistance difference between the two types of polyaspartic polyurea. [7]
| Check objects | Questions to be answered by ingredient information | Questions to be answered in finished product verification |
|---|---|---|
| The main film formationraw materials on both sides are aliphatic or cycloaliphatic polyaspartic polyurea surface layers | What structural categories are used on the polyaspartic ester resin side and the isocyanate side? | How will the color difference, gloss loss, chalking and cracking of the specified color and compatible system behave after specified exposure? |
| Polyaspartic polyurea surface layer with aromatic film formation structure | Which film formation component does the aromatic structure come from, and is it in the directly exposed layer? | Whether the actual color change exceeds the allowable range of the project, and whether there is a verified topcoat if necessary |
| A composite system consisting of an aromatic bottom layer and an aliphatic surface layer. | What are the respective compositions and responsibilities of the bottom layer and the exposed layer? | Whether the covering, interlayer adhesion and aging integrity of the surface layer meet the usage conditions of the part |
When making an inquiry, you can ask the supplier to explain the category of the "main film formation reaction raw materials on both sides" and whether it covers only the exposed surface layer or the entire coating. The scope of "fully aliphatic" in the material name needs to be clear. The formula information of pigments, fillers and additives should be confirmed separately according to technical and contract requirements.
Weather resistance acceptance inspection also distinguishes between appearance and protection function. Slight discoloration of clear topcoat may have a significant impact on appearance-sensitive projects. Even if the color difference of the colored protective film is qualified, cracks, blistering, powdering and necessary adhesion maintenance must be checked. Gaodun's technical judgment is that when selecting outdoor products, you should first agree on which changes will affect delivery, and then select a report that can prove this indicator to avoid extending the single result of "yellowing resistance" to the long-term reliability of the entire system.
What efficiency does quick fixing bring and how to leave enough operating time?
When the temperature, humidity and construction method are suitable, fast-curing polyaspartic polyurea can shorten the time waiting for recoating or open use. The molecular structure around the reaction site of the secondary amine contained in polyaspartic ester resin will affect the speed of its contact and reaction with isocyanate. The Covestro raw materials manual describes different resin grades. Resin selection will affect the operating time and drying speed after mixing. This design space allows builders to select different operating windows for plans, elevations or details. [1]
The project plan must at least separately check the mixing operable time, the earliest and latest recoating time, and the time allowed for rain or open use. The mixing operable time determines whether a batch of materials can be laid out in time, the overcoating window determines how the inter-layer processes are connected, and the opening conditions determine when people can enter or receive water. Surface dry only reflects the status of the membrane surface. Engineering recoating, traffic and water reception have their own conditions, which must be judged according to the corresponding model data and on-site verification respectively.
Ask what “finished today” means in the quotation: application complete, ready to recoat, or ready for traffic. For Gaodun N700, the reference pot life after mixing parts A and B is about 1 hour at 25 °C (Simplified Chinese N700 TDS V2.6, p. 2). Confirm the recoating interval and time to reopen to traffic separately.
How high solids affect film formation thickness and dosage
Under the same wet film thickness, the volume solid content in the construction state is higher, and theoretically a thicker dry film can be formed. ISO 3251 determines the mass proportion of non-volatile substances under specified conditions. ISO 3233-1 uses dry coating film density to determine the volume percentage of nonvolatile matter. It is preferred for air-drying materials and is not applicable to coatings that exceed critical pigment volume concentrations. For reactive two-component products, the applicability of the method, A/B ratio and curing conditions should be checked separately, and then the corresponding data should be used to estimate the construction volume. [4][5]
The mass content is suitable to be determined by the mass ratio under the specified test. To estimate wet film to dry film relationships, applicable volumetric solids data should be used. If the same type of paint is added with diluent on-site according to the approved process, the data in the construction status should be used when estimating. Theoretical values are used to compare plans. Substrate absorption, rough contours, additional details and construction losses must also be considered on site. The formula of high solids must also verify wetting, leveling and venting, especially when constructing at low temperatures or designing a thick single track.
Example | What to look for first when choosing an outdoor clear topcoat
Assuming that the colored decorative layer is to be retained on the south-facing balcony, two clear topcoats are being compared. Both are marked aliphatic, and the first one provides the same weathering effect on the base of the transparent finished compatible system and allows for a recoating window. The second model only gives descriptions of high solids and fast surface dry. At this time, priority should be given to the first model for a compatible system site trial, and at the same time, check whether it is slippery after rain and the actual background color changes. The second paragraph also needs to supplement the color changes, interlayer adhesion and construction window information of the same type of transparent samples. The site trial should choose a location where it is easy to see the change in background color, and keep unexposed reference photos of the same background color.
Conclusion | Implement each advantage into the designated finished product
For outdoor surface layers, first confirm the structural type and the weather resistance of the corresponding finished product. For rush-work scenarios, first confirm how long it can be constructed after ingredients are mixed and when it will be opened. When quoting based on thickness, check the volumetric solid content and target dry film under construction. Only when the three data can correspond to the same finished product, the same compatible system and expected working conditions, the material advantages of polyaspartic polyurea can be used to compare engineering solutions.
References
[1] Covestro (Covestro): "Pasquick® polyaspartic technology. Change the coatings game.", official website technical manual, year of publication not verified, see the chemistry and raw materials combination section. Access date: 2026-11-06. Source PDF (solutions.covestro.com)
[2] Mirreza Gheybi, Abdolreza Mirmohseni, Ali Olad: "Multifunctional fast-curing polyaspartic ester polyurea/PANI-CsC@TiO2 composite coatings with antistatic and anticorrosion properties", Scientific Reports, 2026, 16: 3648. Check the experimental methods in the manuscript accepted by the publisher. Access date: 2026-11-06. DOI (doi.org) Source PDF (nature.com)
[3] BASF: "Basonat® HI 100 NG MB — Technical Data Sheet", July 2023. Access date: 2026-11-06. Source (download.basf.com)
[4] International Organization for Standardization (ISO): "ISO 3251:2019 — Paints, varnishes and plastics — Determination of non-volatile-matter content", 2019 5th Edition. Only the official introduction was checked and the full text of the standard was not read. Access date: 2026-11-06. Source (iso.org)
[5] International Organization for Standardization (ISO): "ISO 3233-1:2019 — Paints and varnishes — Determination of percentage volume of non-volatile matter — Part 1: Method using a coated test panel to determine non-volatile matter and to determine dry-film density by the Archimedes' principle", 2nd edition, 2019. Only the official introduction was checked and the full text of the standard was not read. Access date: 2026-11-06. Source (iso.org)
[6] American Chemistry Council: "Architectural Coatings", official application notes of the aliphatic diisocyanates industry group, undated page. Access date: 2026-11-06. Source (americanchemistry.com)
[7] R. P. Singh, N. S. Tomer, S. V. Bhadraiah: "Photo-oxidation studies on polyurethane coating: effect of additives on yellowing of polyurethane", Polymer Degradation and Stability, 2001, 73(3): 443–446. Only the publisher's abstract and published experimental fragments were checked, and the full text was not read. Access date: 2026-11-06. Source (sciencedirect.com)