POLYASPARTIC TECHNICAL ARTICLES
Polyaspartic Polyurea Technical ArticlesHow Can the Advantages of Polyaspartic Polyurea Be Verified? A Checklist for Weatherability, Adhesion and Outdoor Exposure
To verify whether polyaspartic polyurea is suitable for outdoor use, first check whether the reported sample is consistent with the quoted model and actual construction system, and then look at the exposure conditions of the weather resistance test, the damage location of the adhesion test, and the environment and time covered by the outdoor field exposure record. The number of weather-resistant hours cannot be directly converted into on-site service life. Twenty years of roof waterproofing is the design working life of engineering waterproofing. This article uses a set of simulated quotations to illustrate how to identify evidence gaps and provides a list of information that can be obtained directly from the supplier to help readers distinguish between third-party testing, internal company verification, field records and engineering design information. After getting the report, you can check the sample model, compatible system level, testing conditions and recording date according to the list item by item.
Article contents (9 sections)
To verify polyaspartic polyurea, the first step should be to check whether the sample is consistent with the project
To determine whether polyaspartic polyurea has the advantages of outdoor weather resistance and adhesion, you should first confirm that the report measured the purchased model, corresponding color and coating system to be constructed, and then check the test method, conditions and results. Reports demonstrate how a sample performs under specified conditions. Use it to support roof or terrace selection and determine whether the reported substrate, primer coat and film thickness are representative of the site. Weather resistance, adhesion and outdoor field exposure answer different questions and should be checked one by one according to the engineering purpose. [1][2][3]
First look for the sample page and sample preparation page in the report. Confirm the production unit, complete model, color and compatible system primer coat, and check if there is a batch number or traceability code. Then look for the substrate, surface treatment, number of coating passes, dry film thickness and curing conditions of the sample. The quotation refers to the entire system, but when the report only tests one free coating or a test panel with different substrates, the supplier should be asked to indicate which layer the results only represent and which engineering conditions need to be verified separately.
In a weathering report, what is more important than the number of test hours?
Artificial weathering tests allow observation of material changes under well-documented conditions. ISO 16474-2:2013 specifies xenon arc lamp exposure methods, and its 2022 amendments address daylight filter classification. When comparing reports, the standard version, optical filter, irradiance and corresponding wavelength or band, temperature and humidity, humidity cycle and criteria should be checked. Gaodun's public testing page lists 4,000 hours as corporate laboratory verification, and the corresponding records of specific samples and exposure procedures still need to be checked. [1]
Let’s look at what was measured after the exposure. For transparent or light-colored surface layers, you can pay attention to color difference, yellowing and gloss loss. Colored outdoor protective films should also be checked for chalking, cracking, blistering and adhesion changes based on actual use. If the report only states "no abnormality" or "passed", the other party should be asked to provide the inspected items, evaluation methods, judgment thresholds and judgment basis. The gloss retention rate should be able to check the initial gloss and measurement angle, and the color difference should be able to check the evaluation method and reference. The numerical value can only be used for judgment if it corresponds to the acceptance inspection index of the project.
The length of laboratory exposure is not directly equivalent to the time experienced in the field. The direction of light, duration of wetness, temperature difference between day and night, salinity, pollution and maintenance conditions vary with the project, and the coating may also fail first due to different factors. Q-Lab's technical note states that there is no universal conversion relationship between laboratory testing and actual outdoor years. When comparing two products, you should first confirm that they use comparable specimens, exposure procedures, and failure criteria. [4]
Adhesion depends on both the numerical value and the location of destruction.
In a pull-off adhesion test, force is applied through a loading fixture (dolly) bonded to the coating. The test records pull-off strength and where the specimen failed. ISO 4624 deals with pull-off tests of paints and varnishes. ASTM D7234 is specifically designed for portable pull-off testing of concrete coatings, and explains that the test results are affected by equipment and test specimen conditions. When comparing reports, you should look at single point and summary results expressed in megapascals (MPa), test equipment, sample preparation and curing conditions, as well as cross section and damage type. [2][3]
| Major damage locations recorded in the report | How can we understand | Next step to check |
|---|---|---|
| coating and substrate interface | This test point is mainly damaged along the corresponding interface. | Check substrate moisture content, surface treatment, primer coat and on-site construction records |
| Inside coating or between two coatings | This test point is mainly damaged by the coating itself or between layers. | Find out the specific layers, overcoating windows and compatible systems of each layer |
| concrete interior | This point is destroyed first in the concrete, and the recorded value is affected by the strength of the substrate. | Check the substrate status and sections, and interpret the results according to project rules |
| Adhesive layer bonding the pull-off dolly | The test adhesive layer was damaged first, and the damage strength of the target interface was not measured. | Process according to the method used and acceptance inspection rules, and make additional tests if necessary. |
If there are multiple substrate surfaces on site, the picking points and criteria should be agreed separately. Especially for old ceramic tiles, the smooth brick surface, seam edge and repair area are different interfaces, and the results on concrete cannot directly represent the ceramic tiles. Before performing a destructive pull-off adhesion test on the roof, agree on how to repair the test area and what to reinspect after testing. [2][3]
How outdoor exposure records help judge on-site performance
Outdoor field exposure allows the recorded test panel or engineering area to experience the real outdoor environment and review it at the agreed time point. Compared with laboratory tests, outdoor exposure can provide environmental and usage information in actual locations. Project tracking can also observe details such as drain outlets, ends, and seams. When interpreting, you need to look at the date of the initial and most recent review, the location and orientation, whether it is exposed to direct sunlight, water accumulation or affected by salt spray, the actual film thickness and compatible system, and whether it has been repaired. Only giving a finished photo will not establish a long-term observation record.
Coastal projects should distinguish between general outdoor exposure, salt spray deposition and direct splash. If the roof outdoor exposure record comes from an unobstructed site trial without seawater splash, it can support the judgment in a similar environment. When used on the windward side of the seaside, frequent traffic areas or long-term flooding areas, it should be checked whether these working conditions are covered by records, and supplementary verification should be made according to the gaps. Outdoor exposure tracking can illustrate observed conditions, and records of maintenance, recoating and failures should also be retained.
How to view third-party reports, internal verification, outdoor exposure and design age separately
| Data category | Questions that can be answered | Boundaries to check when purchasing |
|---|---|---|
| Third party testing | How does the sample submitted for inspection perform under the specified methods and conditions? | Check the original report, sample source, method and judgment basis. Distinguish between entrusted sample delivery and independent sampling |
| Internal verification of the enterprise | What is recorded in R&D controls, compatible system screening, or construction windows | Check the sample identity, original records, repeatability and internal judgment basis, and indicate the company’s self-test |
| outdoor field exposure or engineering tracking | Designated site and what happens during observation | Check exposure conditions, review time, location, photos and maintenance records |
| Engineering waterproofing design working years | What age requirements are required for engineering design? | Check the system, details, environment and maintenance conditions used in the design, and separately confirm the contract warranty scope |
Article 2.0.2 of GB 55030—2022 stipulates that the waterproof design working life of roofing projects should not be less than 20 years. This number applies to the waterproofing design of roofing projects. When checking the number of years in the quotation, the supplier should be asked to list the engineering design basis, the waterproofing system used and the contract warranty conditions. Test reports and observed field records can participate in the demonstration, and each is still limited to the conditions covered. [5][6]
Example | Both quotations have reports, which one can better support procurement?
Let’s say two quotes are for the same piece of exposed concrete roofing. Party A provided a xenon lamp report of the gray steel plate sample and a completed photo, but the quotation used a white surface layer, and the report did not provide the compatible system bottom layer of the steel plate. Party B provides data on weather-resistant test panels with the same color and clear compatible system as quoted, and provides adhesion testing of similar concrete compatible system systems, recording the location of damage. If both quotations lack site water content and details site trial information, they should still be verified before starting construction. Among the existing evidence, Party B’s information is closer to the procurement conditions. Party A's report can be used to understand the gray samples tested, and the white finished products and project compatible system need to be verified separately.
Six pieces of information that can be obtained directly from suppliers
- Delivery List. Indicate the complete model, color, primer coat and surface layer of the product, as well as the applicable substrate and film thickness. Attached is the current technical data sheet and version.
- Original report. Request complete, verifiable documentation including issue date, sample page, method page, and results page. Confirm that the samples in the report can correspond to the quotation.
- Weather resistant record. Request the standard version, light source and cycle, exposure time, sample compatible system and dry film thickness, as well as the indicators and judgment basis before and after exposure.
- adhesion records. Request substrate and surface treatment, equipment, test points, strength of each point, damage location and criteria. The repair method will be clarified during on-site inspection.
- outdoor exposure or engineering records. Request the location, start and end dates, exposure method, compatible system, review photos, defect records and maintenance history, and indicate the recording party and verification scope.
- Project files. Check the waterproof design working life basis, details practices, construction process inspection, acceptance inspection plan and contract warranty conditions.
Conclusion | Check the sample and conditions first, then compare the values
When purchasing polyaspartic polyurea, first screen out evidence that does not correspond to the delivered model and system, and then compare the results in reports with comparable conditions. When used on specific roofs, site trials, construction records, and acceptance inspections are used to fill gaps in laboratory evidence. The performance and years in the contract should clearly indicate the corresponding objects and basis.
References
[1] International Organization for Standardization (ISO): "ISO 16474-2:2013 — Paints and varnishes — Methods of exposure to laboratory light sources — Part 2: Xenon-arc lamps", 2013 first edition. Check the official disclosure scope andAmendment No. 1 of 2022: Daylight Filter Classification (iso.org). Access date: 2026-11-06. Source (iso.org)
[2] International Organization for Standardization (ISO): "ISO 4624:2023 — Paints and varnishes — Pull-off test for adhesion", 2023 4th Edition. Only the official introduction was checked and the full text of the standard was not read. Access date: 2026-11-06. Source (iso.org)
[3] ASTM International: "ASTM D7234-22 — Standard Test Method for Pull-Off Strength of Coatings on Concrete Using Portable Pull-Off Adhesion Testers", 2022 edition. Only the official scope of application and significance were checked, and the full text of the standard was not read. Access date: 2026-11-06. Source (store.astm.org)
[4] Q-Lab Corporation: "LU-0833 Correlation Questions & Answers", 2025 updated version. Access date: 2026-11-06. Source (q-lab.com)
[5] Ministry of Housing and Urban-Rural Development of the People's Republic of China: "General Specifications for Waterproofing of Buildings and Municipal Engineering", GB 55030-2022, effective from April 1, 2023. See Section 2.0.2. Access date: 2026-11-06. Source (mohurd.gov.cn) Source (ebook.chinabuilding.com.cn)
[6] Shenzhen Luohu District Construction and Public Works Department: "What are the regulations on the working life of engineering waterproofing design in my country?" ", 2023-09-11. Access date: 2026-11-06. Source (szlh.gov.cn)