POLYASPARTIC TECHNICAL ARTICLES

Polyaspartic Polyurea Technical Articles

Effective Crosslinked Networks in Polyaspartic Polyurea: Why Are Fast Curing and High Hardness Insufficient to Establish Long-Term Durability?

The performance of polyaspartic polyurea depends not only on the conversion of reactive groups, but also on the final network structure formed. Gel, surface dry, hardness establishment and effective cross-linking are not the same concepts. Gaodun combined public research and discussed how to connect the raw materials design, film formation process and long-term protection starting from the reaction path, network defects, the role of soft and hard segments, and structural evolution. When comparing formulas, the curing process, free film performance and the combination of coating and substrate can be recorded separately, and then the performance maintenance after exposure can be checked according to predetermined working conditions to avoid inferring long-term performance from one hardness measurement. Sub-testing can help find out whether performance changes occur during film formation or service.

Article contents (10 sections)

1. Why may the properties of the material be different even after it has been cured?

Polyaspartic polyurea usually forms a urea bond through the reaction of the secondary amine group and the isocyanate group, and the multifunctional components further build a three-dimensional network.

But "film formation" cannot fully describe the network status.

Even if the same type of resin and curing agent are used, different internal structures may be formed due to differences in reaction equivalent, functionality distribution, soft segment composition, mixing and curing conditions.

In this article, according to the Gaodun product label, the isocyanate component is called Part A, and the polyaspartic ester resin component is called Part B. The naming of other companies may be contrary, and the chemical composition description should prevail.

Gaodun believes that material evaluation needs to go through three levels: how much reactive groups are consumed, what network is formed, and what performance the network can maintain in the target environment.

2. What is the difference between reaction conversion rate, gel and effective network?

Reaction conversion rate describes the proportion of a certain type of reactive group consumed.

The gel point describes the critical state at which a continuous network begins to form.

An effective network focuses on which connections can participate in transmitting stress and limiting chain segment movement under specified conditions.

Table 1
concept Main questions answered What cannot be proven independently
reaction conversion rate How much of a certain type of reactive group is consumed? Not established by this evidence alone: Whether all form a target network
gel point When did the through-network begin to form? Not established by this evidence alone: Whether it has been fully cured or reached the use performance
surface dry and hardness Surface state and local response under specified conditions Not established by this evidence alone: Internal cure level and long-term durability
effective network structure How networks connect and function Not established by this evidence alone: Ultimate applicability in all environments

Based on the analysis of polymer network principles, effective connecting chains, dangling chains, intramolecular rings and extractable components may coexist in the film formation system. They contribute differently to load transfer and chain segment motion.

The network defects discussed here are not equivalent to bubbles, pinholes or cracks visible to the naked eye. The former belongs to the molecular connection level, and the latter belongs to the coating morphology level, which requires different identification methods.

Valid networks also have measurement conditions. In addition to chemical cross-linking, hydrogen bond aggregation, entanglement and microphase structure also affect material response at different temperatures and time scales.

3. Why does the reduction of NCO not equal the formation of the same number of effective connections?

Infrared spectroscopy can track changes in the characteristic absorption of the isocyanate group and is an important method for studying the curing process. However, this signal describes group changes and cannot independently restore each reaction path.

In addition to reacting with the target secondary amine, NCO in the actual formula may also react with water or other active hydrogen components. Even if they are all target reactions, different functionalities, local reaction conditions, and intramolecular connections may form different network topologies.

Therefore, the one-to-one correspondence between NCO consumption degree, gel proportion and effective network chain density cannot be established without verification.

Gaodun believes that the reaction spectrum should be mutually corroborated with rheology, gel content, swelling and mechanical analysis. A single piece of data can reveal part of the mechanism, and a complete judgment requires the support of multiple types of evidence.

4. Cutting-edge research reveals: Gel speed and network formation are not simply synchronized

The public abstract of the "Polymer" paper reports that in the formula under study, after adding dibutyltin dilaurate, the gel time is about 7 times that of when no addition was made, and the reaction conversion rate corresponding to the gel point is reduced. Gel time records how long has elapsed, and gel conversion records how far the reaction has progressed by the time the gel point is reached.

The authors analyzed both results using a combination of infrared, nuclear magnetic resonance, mass spectrometry and statistical modeling. The public abstract states that sequential reactions after generating urea bonds can form hydantoin rings, which can also be accompanied by branching and cross-linking. This mechanism corresponds to the formula under study, and the construction pot life needs to be separately evaluated based on the actual formula and usage conditions.

This result suggests that auxiliaries may affect different reaction pathways at the same time. Its effect in polyaspartic polyurea cannot be predicted solely from its common role in other polyurethane systems.

This result corresponds to the formula used in the study and cannot be used as a general adjustment rule for all polyaspartic polyurea, nor can it be directly used as a dosage recommendation.

For Gaodun, construction window optimization should simultaneously observe pot life, film performance establishment, final network and storage stability. When extending the operational time, it is necessary to confirm that the target performance is not adversely affected.

5. Why is a higher degree of cross-linking not necessarily more suitable for all applications?

Increasing the degree of chemical cross-linking can often limit segment motion when other factors come into play, but its impact on final properties also depends on soft segments, hydrogen bonding, microphase structure and formulation composition.

Stronger chain segment constraints may improve creep or solvent resistance under certain conditions, and may also limit deformation and stress release. If the coating does not match the deformation of the substrate, local stresses need to be concerned.

On the other hand, lower network constraints do not automatically mean better flexibility and durability: the material may still face high temperature creep, insufficient media resistance, or insufficient deformation recovery.

Therefore, Gaodun advocates choosing a reasonable degree of network constraints according to the application.

Table 2
Application direction Network design requires coordinated performance
Rooftops and terraces Deformation adaptation, adhesion and waterproof performance after aging
outdoor floor Resistant to scratches, abrasion, impact and interlayer adhesion
Industrial metal protection Shielding, wet adhesion and damage expansion at defects

"High hardness" should be stated together with temperature, curing time and measurement method. It is not a direct substitute for evaluation of wear resistance, impact resistance or long-term corrosion protection.

6. Hard and soft segments collaborate to determine how the network responds to the environment.

For polyaspartic polyurea using isocyanate prepolymers, the soft segments introduced by the polyol participate in regulating the chain segment motion; the hard segments, hydrogen bonds and chemical cross-links jointly affect network constraints.

A 2026 study in Polymers compared reaction behaviour, mechanical properties and water resistance in coatings made with IPDI prepolymers based on PTMEG or PPG. The researchers used a formulated PAE-C coating for the concrete protection tests. Those results apply to PAE-C under the reported test conditions.

This study supports the need for the soft segment to participate in the overall design, but does not identify one polyol as the optimal choice in all formulations.

Gaodun believes that raw materials need to control reaction equivalent, functionality, film thickness and curing conditions, and judge based on glass transition, dynamic mechanics and performance after water absorption.

Otherwise, the influence of the structure of raw materials is easily mixed with changes in test conditions.

7. The network changes over time, and it is necessary to distinguish between post-curing, structural transformation and degradation.

Performance changes after coating film formation may come from continued curing, physical relaxation, chemical structure transformation, or environmental degradation.

Research in "Progress in Organic Coatings" in 2025 shows that in the aspartate polyurea network studied, heat and weak acid can promote the formation of hydantoin rings; its mechanical impact is related to the network structure and the presence of plasticizers. Effect of the formation of hydantoin in aspartate-based polyurea networks (2025, publisher's abstract) (sciencedirect.com)。

Therefore, it cannot be judged that the durability of the material continues to improve just by the increase in hardness over time; nor can all structural changes be classified as aging failure.

A reasonable study should set up unexposed control samples of the same age, and record the curing temperature, humidity and moisture content of the samples. For water-immersed specimens, it is also possible to compare wet and re-dried properties to distinguish recoverable changes from sustained damage.

For example, if the modulus of the same coating decreases after being immersed in water, then basically recovers after drying again, and it still obviously loses adhesion or deformation ability after drying again, different explanations are needed.

8. How to verify that "effective network" indeed improves protection?

Gaodun proposed that structural characterization and application testing should be connected to avoid directly using a certain network parameter as a product performance conclusion.

Table 3
method Main purpose interpretive boundaries
Infrared spectrum Track group changes Network topology cannot be determined alone
Rheological analysis Study gel and modulus establishment Gel criteria and test conditions need to be clarified
Gel content and swelling Analyze insoluble networks and their behavior in response to solvents Affected by solvent, filler and extraction conditions
Dynamic mechanics analysis Observe network response over temperature and frequency Hydrogen bonding, microphase separation, and fillers can affect interpretation
creep and stress relaxation Evaluate deformation and restraint changes under sustained loading Need to correspond to actual temperature and stress conditions
Performance test after aging Examine the impact of structural changes on your application Film thickness, curing and exposure conditions need to be controlled

When estimating crosslink density using swelling or dynamic mechanics, model assumptions need to be checked.

For systems containing fillers, significant microphase separation, or strong physical associations, the estimated value may reflect the joint contribution of multiple constraints and cannot be interpreted without correction as a purely chemical crosslink density.

At the application level, further verification is needed:

  • Metal Protection: Combines electrochemical resistance, wet adhesion and corrosion extension.
  • Roof waterproofing: Combines low temperature flexibility, crack adaptation and waterproof performance after aging.
  • Outdoor flooring: Interlayer stability after combined wear, impact and aging.

9. Gaodun’s technical stance: Let network design correspond to verifiable service performance

Shenzhen Gaodun New Materials Co., Ltd. has focused on polyaspartic polyurea systems since 2016, focusing on the research and development, synthesis, formulation and production of Part A and Part B.

Gaodun believes that the value of network design should be implemented in the consistency of raw materials, response controllability, film formation quality and long-term performance maintenance. The resin and curing agent need to be designed collaboratively; the sample structure needs to correspond to the actual film thickness, construction status and usage environment.

What this article proposes is an R&D evaluation idea, and it does not mean that Gaodun has completed all the characterization or testing in the article. Specific model performance is subject to the corresponding technical instructions and test reports.

For polyaspartic polyurea, questions worthy of continued research are: under the target temperature, humidity and stress conditions, whether the formed network can remain stable, whether the interface can maintain the combination, and whether the coating can continue to exert the required protective effect.

Further reading and technical information

The links below provide background on the topic. When it comes to specific performance, product selection or engineering parameters, please check the applicable objects and test conditions of each data.

The above original data is used to verify the corresponding technical principles, research formulas or construction examples, and is not the testing or certification of Gaodun products. Research conclusions should be understood together with formulas, specimens and test conditions; construction parameters of products from different manufacturers cannot be directly interchanged.