POLYASPARTIC TECHNICAL ARTICLES
Polyaspartic Polyurea Technical ArticlesAromatic and Fully Aliphatic Polyaspartic Polyurea: Assessing Formulation Structure, Weatherability and Service Life
The key difference between aromatic and fully aliphatic polyaspartic polyurea lies in the structure of isocyanate and other raw materials in the main film formation network. The aliphatic and cycloaliphatic routes are generally more conducive to outdoor color retention, but long-term waterproofing and corrosion protection still need to be supported by formula, aging performance and outdoor exposure evidence. This article distinguishes between material structure, research results and Gaodun technical judgment, and explains the selection boundaries of the two types of systems. Aromatic polyaspartic polyurea usually refers to the formula using aromatic isocyanate or its prepolymer such as MDI, TDI, and aspartic acid ester resin to form a reaction system. Even if Group B uses aliphatic source resin, the aromatic structure introduced by Group A will still enter the curing network. The entire system cannot be called fully aliphatic just based on the name of Group B.
Article contents (6 sections)
1. It is also called polyaspartic polyurea. What is the first difference in the formula?
Polyaspartic polyurea is usually film formed by reacting components containing isocyanate group with polyaspartic ester resin. The Covestro Pasquick® technical manual describes the reaction of aspartic acid esters with aliphatic polyisocyanates, as well as the impact of different raw materials on construction and mechanical properties. [1]
This article follows Gaodun’s nomenclature: A is the isocyanate component, and B is the polyaspartic ester resin component. The A and B names of other brands may be opposite and should be identified by chemical composition.
Aromatic polyaspartic polyurea usually refers to the formula using aromatic isocyanate or its prepolymer such as MDI, TDI, and aspartic acid ester resin to form a reaction system. Even if Group B uses aliphatic source resin, the aromatic structure introduced by Group A will still enter the curing network. The entire system cannot be called fully aliphatic just based on the name of Group B.
The "fully aliphatic" mentioned in this article is limited to the main film formation raw materials adopting the aliphatic or cycloaliphatic route, and checking the prepolymer chain segments, resins and other components involved in the film formation; this is a formula description and does not represent a unified weather resistance level, nor does it mean that there are no pigments, fillers, additives or solvents.
| Compare items | aromatic route | fully aliphatic or cycloaliphatic route |
|---|---|---|
| Source of isocyanate | MDI, TDI and corresponding derivatives, etc. | HDI, IPDI, hydrogenated MDI and corresponding derivatives, etc. |
| Group B resin | Aspartate resin can be used | It is also necessary to check the resin skeleton and compatible system |
| Prepolymer design | May contain aromatic hard segments and different soft segments | Still need to check soft segment and other film formationraw materials |
| Exposed design highlights | Pay attention to yellowing and surface aging, and use a weather-resistant surface layer if necessary | It has the advantage of light-resistant design, but still needs complete formula verification. |
| Identity determination | See the specific raw materials and curing network | Don’t just look at “pure”, “imported” or the name of the raw materials supplier |
For the above-mentioned classification of raw materials, please refer to the separate enumeration of aromatic, araliphatic, aliphatic and cycloaliphatic isocyanate in the DIC published patent. [2] The table is a comparison of technical routes, not a formula that can be put into production directly.
It is also necessary to explain XDI separately: Its isocyanate group is connected to the benzene ring through a methylene group, which belongs to the araliphatic group. It cannot be confused with the direct connection method of MDI and TDI, and it should not be classified into the strictly aromatic ring-free fully aliphatic route. [2] The XDI-containing system should be evaluated based on the specific structure and test results. It cannot be concluded that its weather resistance is equivalent to that of the MDI system just because it has a benzene ring.
2. Why does changing the curing agent not just change the name?
The difference between the two formulations is not just the replacement of one type of isocyanate with another.
The isocyanate structure, functionality, NCO content, prepolymer soft segment and Group B resin equivalent will jointly affect the reaction ratio, curing speed, cross-linked network and performance. The Covestro manual lists different resins and curing agents separately, and explains that the selection of raw materials will affect mechanical properties, substrate adhesion and application adaptation. [1]
Therefore, when an aromatic scheme is changed to an aliphatic scheme, it usually needs to be redesigned or checked:
- Reaction equivalent and finished product mixing ratio.
- Application windows, viscosity and leveling.
- Stretch, elongation, hardness and deformation adaptability.
- Pigment and filler dispersion, stabilization system and interlayer compatible system.
- Performance retention after exposure to water, light and temperature.
Gaodun technical judgment: The roof needs to take into account continuous waterproofing, deformation adaptability and exposed durability; the industrial surface layer may also pay attention to hardness, abrasion and media contact. It cannot be assumed that all aliphatic formulas are soft, or that all aromatic formulas are harder and more wear-resistant.
If the prepolymer has already used aromatic isocyanate, adding only part of the HDI curing agent will not eliminate the existing aromatic chain segments. The compounding of aromatic and aliphatic should be truthfully stated as a compound route and verified according to the actual compatible system.
3. What is the difference in weather resistance? First distinguish between yellowing, powdering and functional failure
For coatings that require long-term color retention and a transparent or white appearance, aliphatic and cycloaliphatic isocyanate are often more favorable design starting points. Covestro positions HDI trimer Desmodur® ultra N 3600 as a light-resistant coating curing agent and explains its use in systems with requirements such as weather resistance and gloss retention. [3] This is a description of the use of raw materials and cannot be directly used as a conclusion on the weather resistance of Gaodun finished products.
Photooxidation of aromatic origin structures may form products that absorb visible light, manifesting as yellowing. Singh et al. conducted research on transparent polyurethane formed from castor oil and MDI, reported on yellowing during solarization, and discussed related oxidation products; this time, only the abstract and some experimental fragments provided by the publishing organization were verified. [4]
The subject of this study was aromatic polyurethane and was not a direct controlled trial of polyaspartic polyurea. It supports the explanation of the relevant photooxidation mechanism and cannot be used to assign yellowing time or lifespan to polyaspartic polyurea.
Similarly, "yellowing" cannot be directly equated with "waterproof failure":
- Yellowing mainly describes color changes.
- Gloss loss and powdering reflect surface state changes.
- Cracking, significant embrittlement or delamination may further affect the continuity of protection.
- Whether it is still waterproof or corrosion protection requires corresponding functional testing and on-site evidence.
Mayer-Trzaskowska et al. conducted different aging studies on two commercial polyurethane/polyurea coatings, while investigating surface, structural and adhesion changes. [5] This study uses treated steel substrate and cannot be ranked equally between aromatic and fully aliphatic polyaspartic polyurea, but it does suggest that durability evaluation should cover indicators other than appearance.
Gaodun technical judgment: For projects that have been exposed for a long time and pay attention to color preservation, priority should be given to inspecting the aliphatic or cycloaliphatic main route; at the same time, the adhesion, deformation and protective performance after aging should be verified. Darker colors, pigment coverings, or adding stabilizers cannot automatically prove the long-term stability of the main network; conversely, without adding a certain type of stabilizer, structural inference alone cannot necessarily lead to failure.
4. How many years can aromatic be used, and how many years can fully aliphatic be used?
A fixed number of years cannot be given by material category alone. According to the information verified this time, there is no comparison table between the two types of lifespan applicable to all polyaspartic polyurea formulas, colors, thicknesses and environments.
The evidence requirements are different between "a certain type of material can achieve long-term protection" and "purchasing this model guarantees use for several years." The life span argument needs to clarify at least three levels:
| life span | Need a clear endpoint |
|---|---|
| Appearance service life | What color difference, gloss loss or chalking is allowed? |
| Material functional life | When waterproofing, corrosion protection, adhesion and mechanical properties no longer meet requirements |
| Engineering system age | Usage performance under the combined effects of substrate, details, surface layer and maintenance |
The same coating may change in appearance first, and then affect the function; it may also look good, but leak due to failure of the substrate or details. Therefore, the "color retention life" and "waterproof life" of the two materials cannot be confused.
The Q-Lab technical note states that there is no universal conversion factor between hours of laboratory exposure and years outdoors. When used for comparison, the formula, test cycle, actual exposure location and installation method should be limited, and whether it is comparing weather resistance performance under the same conditions, or whether there is independent outdoor exposure data to study the correlation. [6]
Therefore, 3000 hours or 4000 hours should correspond to the specific light source, cycle, temperature and humidity, film thickness, color and evaluation results. It cannot be directly written as "equal to 15 or 20 years outdoors".
Gaodun technical judgment: The fully aliphatic route can provide a more favorable structural foundation for long-term exposed weather resistance, but 15-20 years can only be demonstrated within the boundaries of specific products, environments and maintenance with sufficient evidence, and cannot be automatically obtained by the four words "fully aliphatic". When the aromatic compatible system is shielded, covered or protected by a weather-resistant surface layer, the complete system should also be evaluated, and the aging judgment of the exposed surface layer cannot be applied.
At present, this article does not make a unified life commitment for the two types of formulas, nor does it judge any Gaodun model as having been proven to achieve a certain long-term life.
5. How does Gaodun transform the advantages of its formula into evidence that consumers can check?
Gaodun advocates establishing a corresponding relationship based on "structural description-finished product verification-actual exposure-engineering maintenance".
First, let’s explain the recipe category clearly. Confirm the source of Group A isocyanate, whether it is compounded, the type of Group B resin and the prepolymer structure. The brand of raw materials can help traceability, but the same international company may provide raw materials with different structures, and the brand name cannot replace the chemical identity.
Second, make the comparison conditions consistent. If you want to compare aromatic, composite route and fully aliphatic, you should try to fix the color, substrate, pre-treatment, dry film thickness, curing and aging conditions, and record the formula adjustments to avoid attributing all the differences in multiple variables to the isocyanate structure.
Again, look at the performance before and after aging at the same time. Evaluate color difference, gloss, powdering, cracks, adhesion and related mechanical and protective properties according to the use; clarify the qualified boundary and damage location. A higher initial index cannot replace durable maintenance.
Finally, keep records of actual exposures and repairs. Only by correlating the sample identity, exposure location, orientation, thickness, photos, inspection and maintenance records can the credibility of life span judgments be gradually improved.
The above is the verification path proposed by Gaodun, which does not mean that all projects have been completed for all models. Unverified formula advantages should be treated as judgments to be verified; Gaodun’s own data should clearly correspond to models and conditions, and results from other companies cannot be borrowed.
When consumers choose long-term exposed polyaspartic polyurea, they can focus on checking three questions: what is the structure of the main film formation raw materials, what evidence of weather resistance performance does the purchased model have, and what are the basis for judging the service life and the applicable conditions. For Gaodun, answering these questions clearly is a concrete way to reflect the value of R&D and manufacturing and long-term protection responsibilities.
References
[1] Covestro (Covestro): "Pasquick® Polyaspartic Technology – Change the Coatings Game", official website PDF version, the year of publication has not been verified, focus on pages 20-21. Source link: Source PDF (solutions.covestro.com)。Access date: 2026-11-01.
[2] DIC Corporation: "ADHESIVE, MULTILAYER BODY, AND PACKAGING MATERIAL", European patent application publication EP4752185A1, 2026, see paragraphs [0016]-[0020]; only the structural classification of raw materials is quoted. Source link: Patent source (data.epo.org)。Access date: 2026-11-01.
[3] Covestro (Covestro): "Desmodur® ultra N 3600", official website product technical information, no version date marked. Source link: Source (solutions.covestro.com)。Access date: 2026-11-01.
[4] R. P. Singh, N. S. Tomer, S. V. Bhadraiah: "Photo-oxidation studies on polyurethane coating: effect of additives on yellowing of polyurethane", Polymer Degradation and Stability, 2001, 73(3): 443-446. This time, only the abstract of the publishing institution and some experimental fragments were verified, and the full text was not read. Source link: DOI (doi.org)。Access date: 2026-11-01.
[5] Paulina Mayer-Trzaskowska, Mariola Robakowska, Łukasz Gierz, Joanna Pach, Ewa Mazur: "Observation of the Effect of Aging on the Structural Changes of Polyurethane/Polyurea Coatings", Polymers, Volume 2024, 16(1): 23, published online in 2023. Source link: DOI (doi.org);Source link: Source (pmc.ncbi.nlm.nih.gov)。 Access date: 2026-11-01.
[6] Q-Lab Corporation: "LU-0833 Correlation Questions & Answers", 2025 updated version. Source link: Source (q-lab.com)。Access date: 2026-11-01.