POLYASPARTIC TECHNICAL ARTICLES

Polyaspartic Polyurea Technical Articles

Can Polyaspartic Polyurea Protect Coastal Steel Structures? From Salt Spray Testing to Complete Corrosion Protection Systems

Salt spray hours alone cannot predict the service life of coastal steelwork. This guide shows how to distinguish atmospheric, splash, tidal and immersion exposure, check each coat’s role and compare evidence for the complete coating system. A dockside example covers welds, edges, drainage and repairs. Use the same component identifiers on drawings, purchase orders and inspection records, and distinguish initial acceptance from inspections during service.

Article contents (9 sections)

Coastal steel structures can use polyaspartic polyurea, provided the system matches the environment

Salt spray hours cannot predict the service life of a coastal steel structure. The report describes how the specified coated test panels performed under the stated salt spray conditions. [3] For a project, first identify the exposure zone: marine atmosphere, splash, tidal or immersion. To consider a polyaspartic topcoat on exposed steel, check the surface preparation, primer and intermediate coat, and confirm that the complete coating system has been evaluated for that exposure. Set maintenance intervals using the condition and service history of the actual steelwork. [1][2]

Why steel parts at the same seaside may require different compatible systems

Steel structures closer to the sea still have different exposure conditions. Windward locations may frequently experience salt deposition. Although sheltered areas are less exposed to direct sunlight, they may accumulate contaminants because they are difficult to flush. The lower part of seaside equipment may also be exposed to splashing, periodic water exposure or accumulation of water. Environmental classification should be confirmed based on actual exposure, location and project applicable documents. ISO 12944-2 classifies the service environment for steel structure protective coatings, including the classification basis for atmospheric corrosion categories and immersion environments. [1]

ISO 12944-9:2018 covers offshore and related carbon steel structures in CX marine atmospheres or Im4 immersion in seawater or brackish water. The official summary states that it is applicable to relevant structures with steel thickness of at least 3 mm. Pipelines and tank inner walls are not within the scope of the document. Coastal building steel parts should first be classified according to actual exposure conditions, and then confirm the complete compatible system and acceptance inspection basis used in the contract. [2]

Table 1
Engineering exposure clues Priority failure risks Compatible system evidence required
Sheltered or exposed steel in a marine atmosphere Risk: salt deposits, rust where the coating is damaged, and weathering of the exposed topcoat. Evidence to check: the exposure classification and weathering and corrosion results for the complete coating system.
Repeated wetting by splash, tides or standing water Risk: prolonged wetting of the coating and corrosion of the steel at edges or coating defects. Evidence to check: system suitability for the actual wetting conditions, detailing and inspection records.
Prolonged immersion Risk: continuous contact with the liquid and possible incompatibility with the coating. Evidence to check: documented suitability for immersion in the specified liquid and the project design basis.

When a component spans multiple water-receiving areas, the boundaries and transitions between different compatible systems should be marked on the drawings. Purchase orders and acceptance inspection records should also use the same part number.

What is polyaspartic polyurea responsible for in the corrosion protection compatible system?

Changing the primer or reducing the number of coats puts the proposed system outside the original assessment. Obtain evidence for the revised system on the proposed steel substrate, with the specified surface preparation, coat sequence and exposure conditions. The primer must suit the prepared steel. The intermediate coat can add barrier protection and film thickness. The exposed topcoat provides the specified weather resistance, colour and surface protection. [2]

If the supplier recommends direct coating of steel, ask its report whether the same model without primer is indeed used, and check the steel material, processing method, roughness, film thickness of each layer, curing conditions and evaluation results. If the reported sample contains primer, the corresponding combination is proved. If the primer, overcoating interval or paint needs to be changed on site, compatibility and verification requirements should be checked according to the project change procedure.

What problems can the number of salt spray hours indicate?

ISO 9227:2022 specifies equipment and procedures for neutral salt spray (NSS), acetic acid salt spray (AASS) and copper accelerated acetic acid salt spray (CASS). Product-specific test specimens, exposure times, and result interpretation are determined according to the corresponding product specifications. The salt spray test can be used to find certain coating defects and check quality consistency. The results alone cannot be used to rank the corrosion resistance of different materials or predict long-term durability. [3]

Read a scribed steel panel report in two places. At the scribe, check the recorded spread of corrosion from the cut and the method used to rate it. Away from the scribe, check the reported blistering and rusting on the intact coating. Identify the substrate, primer, complete coating system and measured dry film thickness on the test panel. For UV exposure, wet–dry cycling or immersion, request evidence specific to those conditions. [2][3]

For a coastal steel component, record the exposure zone and map previous repairs and the condition of welds, bolt heads and areas of standing water. A salt spray report describes the tested panels under specified conditions. Test hours alone do not establish the component’s service life in the field (ASTM B117-26a, section 3.2 (store.astm.org)).

How to do steel surface treatment and edge acceptance inspection

Before painting, the appearance of rust removal, surface contour, dust, soluble salts and condensation conditions should be recorded separately. ASTM D4417 is used for surface profile measurements of blast cleaned steel. [4] The Bresle method in ISO 8502-6 is used to extract water-soluble contaminants from the surface, while ISO 8502-9 uses the conductivity method to evaluate the surface density of soluble salts. The results obtained cannot quantify components such as chloride and sulfate respectively. [5][6] Acceptance inspection should check the measuring points, results and allowable limits according to the project regulations, and keep a record of the time from surface treatment to painting.

Welds, sharp edges, openings, bolts and lower edges of components are areas that require individual attention. If the project requires pre-coating or partial coating, the material, scope and level should be clearly defined, and then the continuity with subsequent coating should be checked. When the average film thickness meets the requirements, the edges may still be thin. The acceptance inspection should cover both the main surface and details according to the points and methods agreed on the project, and record the scope of subsequent repairs.

Example | Exposed guardrails and low-level steel parts near the pier

For low steelwork that is often wet, establish the source of wetting on site: splash, wash water or standing water. Record how often the component gets wet and whether the water persists. Request evidence that the proposed complete coating system has been evaluated for those exposure conditions. Assess a higher guardrail separately if its main exposure is atmospheric. Evidence for the guardrail covers only the substrate and exposure stated in that evidence.

The quotation comparison should list surface cleaning, edge treatment, film thickness of each film, inspection method and maintenance location in the same table. When one company quotes the entire compatible system and the other only quotes the topcoat unit price, the missing items should be filled in before comparing. If the primer is subsequently changed or the process is adjusted, the changes should be written into the construction record and delivery list.

How to create executable maintenance records for steel parts

Inspection records should first list component partitions, inaccessible locations and historical repair points. During the initial acceptance inspection, the main welds, bolts and low water accumulation points can be photographed and numbered. Follow-up inspections followed the same sequence to record areas of localized rust, discoloration, film damage and loss of adhesion. When damage is discovered, cleaning, collisions and recent construction should also be recorded to facilitate the determination of whether the damage is caused by environmental accumulation or mechanical damage.

Before repair, it is necessary to determine whether the old coating is firm and whether there is salt accumulation in and around the exposed steel area. For peripheral coatings that are still strong, cleanliness, edge treatment and compatibility should be checked before overlapping. If rust spreads along the bottom of the coating, first check the expanded range, and then restore each coating according to the project requirements. After the repair is completed, the film thickness, detail coverage and opening conditions should be reviewed against the original design records to avoid treating different parts of the original protection system as one topcoat.

For the purchaser, the quote may also include accessibility for inspection and repair. Higher-level steel parts may require additional access, and lower-level steel parts may be subject to equipment outage windows. Putting these conditions together with the compatible system construction time, we can compare the initial quotation and subsequent maintenance investment under the same service scope. Agreeing on the location and responsible person for the first inspection will help convert the supplier's compatible system description into an executable maintenance plan.

Conclusion | Steel protection is selected based on the entire system

When choosing polyaspartic polyurea for coastal steel structures, you should start from the environment and location, check steel surface treatment, compatible system coating and risk-based tests. The construction acceptance inspection records the main surface film thickness, weld edges and repaired areas separately. Only when testing and field conditions can be matched, material merits can be used for engineering comparisons.

References

[1] International Organization for Standardization (ISO): "ISO 12944-2:2017 — Paints and varnishes — Corrosion protection of steel structures by protective paint systems — Part 2: Classification of environments", 2017 2nd Edition. Only the official introduction was checked and the full text of the standard was not read. Access date: 2026-11-06. Source (committee.iso.org)

[2] International Organization for Standardization (ISO): "ISO 12944-9:2018 — Paints and varnishes — Corrosion protection of steel structures by protective paint systems — Part 9: Protective paint systems and laboratory performance test methods for offshore and related structures", 2018 edition. Only the official introduction was checked and the full text of the standard was not read. Access date: 2026-11-06. Source (iso.org)

[3] International Organization for Standardization (ISO): "ISO 9227:2022 — Corrosion tests in artificial atmospheres — Salt spray tests", 5th edition in 2022, with amendment No. 1 in 2024. Only the official introduction was checked and the full text of the standard was not read. Access date: 2026-11-06. Source (iso.org)

[4] ASTM International: "ASTM D4417-21 — Standard Test Methods for Field Measurement of Surface Profile of Blast Cleaned Steel", 2021 edition. Only check the official scope of application and significance. Access date: 2026-11-06. Source (store.astm.org)

[5] ISO: ISO 8502-6:2020, extraction of water-soluble contaminants for analysis (Bresle method). Check official public summary.ISO official description (committee.iso.org)。

[6] ISO: ISO 8502-9:2020, On-site determination of water-soluble salts by conductometric method. Check official public summary.ISO official description (iso.org)。