POLYASPARTIC TECHNICAL ARTICLES
Polyaspartic Polyurea Technical ArticlesLong-Term Deformation Stability of Polyaspartic Polyurea: From Single Tensile Loading to Creep, Stress Relaxation and Cyclic Fatigue
A single tensile test describes one loading event. To assess creep, track deformation over time under constant load. To assess stress relaxation, track stress over time at constant strain. To assess fatigue, apply repeated loading at a specified amplitude and temperature and inspect for damage. Roof crack-bridging claims also require evidence for the installed system and joint detail.
Article contents (9 sections)
1. One-time tensile performance, why can’t it fully describe the long-term deformation ability?
Tensile strength and elongation at break are important starting points for understanding the mechanical properties of polyaspartic polyurea. However, such results correspond to the specified specimen, temperature, loading speed and curing state.
To assess a roof membrane over a gap that opens and closes, check system tests representative of the substrate and build-up. Record movement amplitude, temperature and cycle count, then check watertightness and debonding. A single tensile test on a free film cannot answer these questions.
Whether a material can remain intact under these conditions cannot be judged solely by the results of a single stretch to rupture.
Gaodun believes that long-term deformation evaluation should further answer: Will it gradually deform after continuous stress? How does the stress change when it is held at a certain deformation position? Does damage occur after repeated deformation?
These three questions point to creep, stress relaxation and cyclic fatigue respectively.
2. What is the difference between creep, stress relaxation and cyclic fatigue?
| behavior | Typical test control methods | Key observations |
|---|---|---|
| creep | Maintain load or stress under specified conditions | Growth of deformation over time |
| stress relaxation | Maintain the specimen at specified deformation | Change in stress required to maintain this deformation |
| Cyclic response and fatigue | Repeated application of load or displacement | Stiffness changes, residual deformation and cracking in the specimen. Under the specified cyclic load or displacement, record the number of cycles to the stated failure criterion. Service life in years requires separate evidence. |
| Uninstall recovery | Continue to observe after removing the load | Instant recovery, delayed recovery and residual deformation |
These behaviors are related to each other but are not substitutes for each other.
The deformation that has not yet recovered after the material is unloaded may include unfinished viscoelastic recovery, damage or irreversible changes. Therefore, "permanent deformation" needs to correspond to the specified recovery time and determination method.
Likewise, softening in the early stages of the cycle is not necessarily fatigue failure and may also involve structural adjustments. Determining damage requires a combination of cracks, performance maintenance and subsequent changes.
3. What structural factors does the viscoelasticity of polyaspartic polyurea come from?
Can a single tensile test describe long-term creep, stress relaxation and fatigue? No. Creep requires a deformation history under constant load, stress relaxation requires a stress history at constant strain, and fatigue requires repeated loading and inspection for damage. Identify the specimen and temperature for each test.
When the stress time is extended, some chain segments may gradually adjust; when the temperature changes, the activity levels of different motion processes will also change. This makes the material modulus and recovery behavior time-dependent.
To compare tensile creep in two cured films, record deformation over time at comparable loads and temperatures. Check specimen dimensions, conditioning and loading duration before comparing curves. A hardness reading cannot replace a creep record.
For Gaodun, the prepolymerized structure of Part A, the molecular structure and reaction equivalent of Part B need to be jointly designed. Flexibility, load-bearing stability and interface stress should be balanced under the target use conditions.
4. Why do high temperature, long time and fast loading give different conclusions?
The same coating may appear harder when loaded quickly; it may deform more when loaded slowly or held for a longer period of time. Temperature changes also alter chain segment motion and material response.
Therefore, the results obtained by rapid stretching at room temperature cannot directly represent the long-term stress performance of high-temperature surfaces in summer.
ISO 899-1:2017 covers plastic tensile creep and emphasizes that specimen preparation, dimensions, environment and thermal history can affect results. This method is mainly suitable for rigid and semi-rigid plastics. Flexible polyaspartic polyurea coatings need to confirm the applicability of the method. Part 1: Tensile creep
Time-temperature equivalence relationships can be studied in research and development to assist in understanding behavior on longer time scales. However, before application, it is necessary to verify whether the same mechanism is maintained under different conditions and to identify the effects of post-curing, aging and non-linear deformation.
Extrapolating short-term high-temperature data to multi-year use requires clear models, applicable scope and independent verification.
5. Does the faster the stress relaxation mean the better the material?
To measure stress relaxation, hold specimen strain constant and record stress over time. The curve describes that specimen at the stated temperature. To determine whether the coating has detached from its substrate, inspect the interface of a bonded specimen.
But relaxation speed is not an indicator of merit that can be pursued alone.
For coatings that need to maintain shape or withstand local pressure, excessive time-dependent deformation may affect use; for protective layers that withstand substrate displacement, sufficient deformation coordination capabilities are required.
More importantly, the stress drop may result from normal viscoelastic adjustment or may be accompanied by cracking or interface debonding. These causes cannot be distinguished by looking at the load drop curve alone.
Gaodun believes that stress relaxation should be evaluated together with appearance, interface integrity and uninstall recovery to understand its engineering significance.
6. The number of cycles is the same, why can’t the fatigue ability be directly compared?
Cyclic testing requires description of deformation amplitude, average strain, frequency, waveform, temperature and loading method.
To compare cyclic tests, check which variable was controlled (load or displacement), then compare amplitude, rate, temperature and cycle count. Record where damage occurred and how failure was defined. Equal cycle counts alone do not establish which specimen has better fatigue resistance.
When the frequency is too high, you also need to pay attention to the temperature rise of the material itself. The dissipated heat generated by repeated deformation may change the actual specimen temperature and cause the test to deviate from the original conditions.
EOTA assessment document EAD 030350-00-0402 covers liquid-applied roof waterproofing kits, including polyaspartic systems. Section 2.2.8 tests resistance to fatigue movement on a fully bonded, assembled system at −10 °C using Annex A4.5. The number of cycles depends on the kit category. After cycling, the system must remain watertight and any debonding must be recorded.
This framework illustrates that repeat displacement should be judged in conjunction with system performance; it does not imply that any polyaspartic polyurea product has passed the corresponding evaluation.
7. What evidence can dynamic mechanics analysis provide?
Dynamic mechanical analysis can help observe the response of materials under certain temperature, frequency and deformation conditions, often focusing on storage modulus, loss modulus and loss factor.
These data help analyze material stiffness, energy dissipation and transformation behavior, but cannot be directly equated to fatigue life.
ISO 6721-1:2019 gives the principles for dynamic mechanical testing of rigid plastics in the linear viscoelastic range, and points out that the results of different deformation modes may not necessarily be directly comparable. Specific flexible coating research also requires the selection of suitable fixtures, amplitudes and sample conditions. Part 1: General principles
| R&D issues | Possible evaluation paths | The results that need to be combined |
|---|---|---|
| Is the deformation due to high temperature load too large? | Multi-temperature, multi-load creep and recovery | Thickness, residual deformation, appearance |
| How does stress change after substrate displacement? | Fixed deformation stress relaxation | Interface and membrane integrity |
| Can protection be maintained through repeated opening and closing? | cyclic displacement of specified amplitude | Cracks, adhesion, water tightness |
| How temperature sensitive is the formula? | Dynamic mechanics and actual deformation testing | Performance maintenance under applicable temperature |
| Whether it can still coordinate deformation after aging | Control test before and after aging | Strength, recovery and injury location |
The above content is a research and development path, and specific product conclusions should be supported by data under corresponding conditions.
8. Gaodun’s research and development direction: evaluate the material ontology and the actual interface together
Free film testing is useful for comparing material structures, but the coating is constrained on the substrate and the local strain distribution may be different from that of the free film.
Free-film elongation at break cannot be converted into an allowable roof crack width. Annex A4.5 of EAD 030350-00-0402 assesses fully bonded waterproofing systems over substrate gaps that open and close. Its scope excludes expansion joints. Check the joint type, detail, expected movement and test evidence for the proposed system.
The evaluation path that Gaodun focuses on is to first understand the time and temperature response through the material body test, and then verify it on the clear substrate, thickness and system structure.
For roofs, attention should be paid to watertightness and adhesion after cyclic displacement; for floors, attention should be paid to indentation and recovery after sustained pressure; for equipment coatings, substrate deformation and actual environmental selection tests should be combined.
Gaodun believes that the value of independent research and development and collaborative design of Part A and Part B should be further implemented into the explanation and control of these long-term behaviors.
The long-term deformation stability of polyaspartic polyurea needs to be proven by the results of sustained stress, unloading recovery, cyclic damage and system protection.
Further reading and technical information
The links below provide background on the topic. When it comes to specific performance, product selection or engineering parameters, please check the applicable objects and test conditions of each data.
- ISO 899-1:2017: Plastic tensile creep and applicable specimens (iso.org)
- EOTA: EAD 030350-00-0402 Liquid Roofing Waterproofing System Evaluation Document (eota.eu)
The above original data is used to verify the corresponding technical principles, research formulas or construction examples, and is not the testing or certification of Gaodun products. Research conclusions should be understood together with formulas, specimens and test conditions; construction parameters of products from different manufacturers cannot be directly interchanged.