POLYASPARTIC TECHNICAL ARTICLES

Polyaspartic Polyurea Technical Articles

How Does Polyaspartic Polyurea Resist Cleaners, Oil and Fertilizer Runoff? Assessing Chemical Resistance

The chemical resistance of polyaspartic polyurea should be judged according to the specific product, contact material, concentration, temperature, time and curing conditions. Routine cleaning of a home patio, occasional oil stains in a garage, and constant chemical exposure in industrial areas cannot be judged by the same criteria. Gaodun believes that when selecting materials, the protective performance, appearance requirements and cleaning and maintenance methods should be explained at the same time to reduce misunderstandings and rework during use. When checking the data, the actual cleaning agent or contaminant, contact time and cleaning method should be stated, and slight discoloration, gloss loss and reduced protective function should be distinguished. Different compatible systems and usage environments should be verified separately. A representative site trial can also be used to check the appearance after cleaning.

Article contents (6 sections)

"After painting polyaspartic polyurea on the terrace, can I mop the floor with detergent?" "Will the fertilizer water flowing out of the flower pots hurt the coating?" "There is engine oil dripping in the garage. Will there be any marks after wiping it off?"

These questions are more specific than "acid and alkali resistance, oil resistance" and closer to the real needs of consumers.

For Gaodun, the description of chemical resistance should let consumers know what the material is suitable for contact with, how to contact it, and how to handle it after contact. Only by clearly explaining the usage conditions can the material advantages be transformed into reliable performance in daily use.

1. Why does polyaspartic polyurea have chemical resistance potential? Structural advantage requires formulation verification

Polyaspartic polyurea forms a cross-linked network after curing. The resistance to different media can be adjusted through the selection of resin and curing agent, reaction ratio and formula design.

In the case of Covestro's Pasquick® application at the Era Polymers production site, chemical resistance, quick drying, durability, anti-skid and other requirements were included in the floor requirements. This shows that polyaspartic polyurea technology has an application foundation for related industrial floors, but actual application still needs to be combined with a specific compatible system. Covestro

When chemicals come into contact with coatings, effects may include penetration, swelling, softening, surface changes, or structural damage. Different media have different effects on the same coating, and the same media may produce different results under different conditions.

Therefore, aliphatic structures, higher hardness or high solids alone cannot prove the same resistance to all cleaning agents, oils and acidic and alkaline media.

Gaodun advocates combining formula design with actual contact verification. Roof waterproofing, home terraces and industrial protection can propose different performance goals; "the same polyaspartic polyurea" does not mean that the scope of chemical resistance is exactly the same.

2. Why are there two usage conditions: short-term splashing and long-term immersion?

Chemical resistance requires the combination of at least five pieces of information: medium, concentration, temperature, time, and the curing state of the coating. **

For example, a cleaning agent diluted according to instructions and then scrubbed for a short time cannot be considered the same contact as a concentrated solution left on the ground overnight. Occasional oil dripping in the garage should be cleaned up promptly, and long-term oil accumulation under the equipment also needs to be judged separately.

Chemical resistance evaluation requires clarifying the medium, concentration, contact method and time. ASTM D543 provides a reference for the evaluation of plastic resistance to chemical reagents. The scope of application and specific coating items must still be verified separately and cannot be directly regarded as the performance of Gaodun products.ASTM D543-21 Official Summary (store.astm.org)。

Table 1
Conditions that need to be clarified meaning for judgment
What substances are exposed to Cleaners, cooking oils, fuels and solvents are not substitutes for each other
Actual usage concentration The action conditions of original solution, working solution and residue are different
contact temperature Thermal cleaning and normal temperature wiping need to be confirmed separately.
How long does it last and how often does it happen? Occasional spills and repeated cleaning are different from continuous soaking
Whether the coating has completed the required curing Surface dry or walkable does not mean it has reached chemical resistance conditions.

The actual mixture also needs attention. The test results of a single chemical cannot directly represent commercial cleaners containing surfactants, solvents, fragrances and other ingredients.

Providing the name, label and usage of the cleaning agent when purchasing is usually easier to get a targeted answer than just asking "can it withstand alkali?"

3. What should we pay attention to when it comes to detergents, oil stains, and flower pot fertilizers and water?

Cleaner: Focus on the complete formula and cleaning method.

Descalers, degreasers, and disinfectants have different ingredients and uses. Just because they are all used at home does not mean they are gentle on coatings by default. It should be used according to the confirmed product type, dilution ratio, contact time and cleaning method.

Scrubbing tools can also affect results. Strong cleaners combined with hard brushes, abrasive pads, or frequent scrubbing can cause both chemical and mechanical effects.

Oil contamination: Focus on distinguishing the types of oil and contact methods.

Edible oil, engine oil, fuel, hydraulic oil and solvent-containing cleaning fluid are not the same medium. Short-term tolerance to a certain engine oil cannot replace judgment on the suitability of gasoline or glue remover.

It should also be distinguished between "the oil stain can be wiped off" and "the performance of the coating film has not changed". Transparent or light-colored surfaces require high appearance; timely cleaning can help reduce residence time and the spread of contamination.

Fertilizer and water for flower pots: focus on composition, drainage and repeated residue.

The formulas of different fertilizers and nutrient solutions vary greatly, and the effluent may be mixed with soil and organic matter. It cannot be generally concluded that all are safe or all harmful.

If the bottom of the flower pot is wet for a long time and fertilizer water accumulates repeatedly, it will be different from the timely drainage after occasional watering. After the clean water evaporates, non-volatile substances may remain, and the actual contact status will change over time.

Gaodun recommends that when selecting a model, indicate whether flower pots will be placed on the terrace for a long time, whether fertilization is applied, and whether cleaning is convenient; maintain drainage during use, clean up residues in time, and check the coating under the flower pots as needed.

4. Are surface imprints, gloss loss and coating damage the same thing?

No. Chemical resistance evaluations need to describe the changes observed and how these changes impact the intended use.

Table 2
Behavior after contact Should be further confirmed
stains or staining Whether it can be removed and whether it affects the decoration requirements
Changes in gloss or texture Whether the cleaning method is suitable and whether the surface is worn or softened
Tacky, noticeably softening or swelling Whether the performance of the coating film is affected and whether it needs to be repaired
blistering, cracking or delamination Whether coating continuity, interlayer or substrate bonding is damaged

Just a change in color cannot directly determine that the waterproofing has failed; similarly, if there is no obvious change in the surface, it cannot be used to prove that long-term adhesion and mechanical properties are not affected at all.

Sherwin-Williams' resin floor maintenance guide reminds that some cleaning agents may affect the color, gloss or texture of the polymer floor. It is recommended to conduct a small area verification first in conjunction with the actual cleaning method. Sherwin-Williams

For Gaodun, verification should observe both appearance and function according to use. Visible stain and shine are important for home decking, while adhesion, hardness or other property retention may also be of concern for industrial areas.

Small-area trials are suitable for screening obvious incompatibilities and cleaning effectiveness, but they cannot replace special verification of long-term immersion or industrial chemical conditions.

5. How can consumers choose and maintain products to reduce unnecessary damage?

Before purchasing, please provide the actual contact conditions to the manufacturer.

Describe the purpose of the site, possible exposure to cleaning agents, oils or fertilizers, as well as frequency of use, temperature and dwell time. For continuous chemical contact, more complete media information should be provided to confirm the specific compatible system.

Check whether the data belongs to the purchased product.

Raw materials technology cases, chemical resistance results of other models or other companies can help to understand the technical direction, but they cannot be directly used as an applicable conclusion for a certain Gaodun finished product.

The information should also describe the test conditions and evaluation implications. Whether "tolerance" means no obvious appearance changes, or whether certain color changes are allowed but performance is maintained, should be clearly expressed.

After completing the required curing, enter the corresponding use.

Whether it can be walked, whether it can be cleaned, and when it can be exposed to chemical media should be judged according to the product requirements. Don't immediately treat the new coating with a strong cleaner just because it's not sticky.

Establish an appropriate cleaning routine.

Within the scope that has been confirmed to be applicable, remove sand and solid dirt first, and then use cleaning agents and tools approved by the compatible system. For the first-time cleaning solution, try it out in an inconspicuous place, clean it and observe it; adjust the method if any abnormalities are found.

If there is a change, judge first and then fix it.

Record contacts, dwell times, cleaning operations and scope of changes for analysis by technicians. If there is softening, blistering or delamination, it is not advisable to cover it directly with new topcoat. The scope of damage and repair conditions should be confirmed first.

Gaodun believes that the chemical resistance value of materials is reflected in its performance and maintainability under specific conditions. By matching products, contact conditions, evaluation results and maintenance methods, consumers can more confidently choose the polyaspartic polyurea solution that is suitable for their terrace, garage or industrial area.

Further reading and technical information

The links below provide background on the topic. When it comes to specific performance, product selection or engineering parameters, please check the applicable objects and test conditions of each data.

The above original data is used to verify the corresponding technical principles, research formulas or construction examples, and is not the testing or certification of Gaodun products. Research conclusions should be understood together with formulas, specimens and test conditions; construction parameters of products from different manufacturers cannot be directly interchanged.