Gaodun N300 or N700 for Roof Waterproofing: The 1.2 mm TDS Reference and a 1.5 mm Budget Example

For primary waterproofing on concrete or tiled roofs and terraces, prefer N300 for prolonged outdoor exposure. Consider N700 for standard weathering requirements. Both technical data sheets give a reference total of 1.3 kg/m² for about 1.2 mm of cured film. This guide uses 1.6 kg/m² for a 1.5 mm target as a budgeting example pending technical confirmation. Verify the relationship by design and a site trial. Neither data sheet compares wear or service life at these two thicknesses. The guide covers purchase quantities, retained tiles and the evidence needed for service-life claims.

Article contents (9 sections)

For primary waterproofing on concrete roofs, tiled roofs and terraces, Gaodun recommends considering N300 first for prolonged outdoor exposure. Consider N700 where standard weathering resistance is sufficient. Both technical data sheets (TDS) give an approximate film thickness of 1.2 mm. This guide also examines 1.5 mm as a project budgeting example. Have the designer confirm the build-up and use a trial area to check consumption against the measured thickness. The 1.5 mm target is for budgeting only. Neither grade’s TDS compares abrasion loss or service life at 1.2 mm and 1.5 mm. Investigate hollow or loose tiles, moving cracks and persistent moisture beneath the surface before deciding whether to retain the tiles.

Choosing N300 or N700 for the exposure

For an exposed roof subject to sustained sunlight and rain, particularly where access for maintenance is difficult, request a quotation for N300 and check the proposed system. For a roof with standard weathering requirements, consider N700 after establishing sunlight exposure, drainage, frequency of use and substrate condition. These are Gaodun’s selection recommendations. To compare the grades at equal thickness, obtain reports for comparable colours, film thicknesses, coating systems and test conditions.

Covestro’s Pasquick® technical brochure explains how polyaspartic esters react with aliphatic polyisocyanates to form a coating and how hardener selection affects mechanical properties, adhesion and application.[1] This chemistry provides a formulation route for exposed coatings, but individual formulations can behave differently. For concerns about discolouration, chalking or cracking, check weathering data for the finished coating at the specified film thickness. For leak protection, also check adhesion, detailing and acceptance of the completed waterproofing system.

Comparing the 1.2 mm reference with a 1.5 mm budgeting example

The desktop TDS for N300 (V2.6, page 3) and N700 (V2.6, page 2) both give a reference total of 1.3 kg/m² across all coats for an approximate film thickness of 1.2 mm. The additional example of 1.6 kg/m² for a target of 1.5 mm is a budgeting assumption. The two current data sheets do not specify that relationship; it requires technical confirmation. Consumption here is the combined mass of Parts A and B in the primary waterproofing layer, and thickness refers to the cured layer. Itemise primer, local reinforcement, a separate topcoat and additional losses according to the project specification.

Table 1
Swipe to see more columns
Grade and basis Total consumption across coats Film thickness Selection conditions
N300, TDS reference 1.3 kg/m² Approximately 1.2 mm Prolonged outdoor exposure; substrate and details must suit the design.
N300, budgeting example pending technical confirmation Assumed 1.6 kg/m² Target 1.5 mm; verify by measurement Consider N300 for prolonged exposure. The 1.5 mm target is a budgeting assumption subject to design review and a measured site trial.
N700, TDS reference 1.3 kg/m² Approximately 1.2 mm Standard weathering requirements; main area and details must suit the design.
N700, budgeting example pending technical confirmation Assumed 1.6 kg/m² Target 1.5 mm; verify by measurement Consider N700 for standard weathering requirements. The 1.5 mm target is a budgeting assumption subject to design review and a measured site trial.

The difference between 1.2 and 1.5 mm is nominally 0.3 mm. That 0.3 mm is the difference between two target thicknesses. Neither the N300 nor the N700 TDS compares wear or service life at these thicknesses. For a roof subject to foot traffic, check the abrasion data and protective layer specified for the proposed system. Applying more material over the roof field cannot make up for thin spots at internal corners, external corners, terminations or drains. Separate the field thickness, detailing and acceptance criteria in the quotation. Average consumption can conceal local omissions.

Comparing the N300 reference of about 1.2 mm with an N700 project target of 1.5 mm involves two decisions: grade and thickness. For an exposed roof, select the grade for the weathering requirement, then confirm the thickness against the design and acceptance criteria. For a trafficked terrace, separately assess slip resistance, abrasion resistance and any protective layers required.

What a diffusion model can tell us about thickness

Increasing the thickness of an intact film generally increases the distance water must diffuse through the polymer. The cited review discusses early Fickian water uptake in epoxy coatings. For the same material, diffusion coefficient, temperature and boundary conditions, the model predicts that the time to reach a given early fractional uptake scales with the square of film thickness. This illustrates the effect of thickness in the model. The study did not measure water uptake or roof service life for N300 or N700.[2]

For 1.2 and 1.5 mm, the theoretical ratio is (1.5 ÷ 1.2)², approximately 1.56. It applies only to the modelled time to reach that fractional water uptake. The cited paper concerns epoxy coatings and did not determine diffusion coefficients or outdoor failure thresholds for Gaodun N300 or N700. The calculation does not predict the life of either roof coating.

A roof may fail at details long before diffusion through the bulk film becomes decisive. Water can enter at a poorly sealed outlet. Moisture beneath a coating can cause blistering or delamination. Movement in a substrate crack can split the film locally. Neither product data sheet gives comparative colour-retention or chalking results at different film thicknesses. Establish where and why water is entering before choosing a thicker construction.

Interpreting 20-year and 25-year statements

Clause 2.0.2 of China’s GB 55030-2022, General Code for Waterproofing of Building and Municipal Engineering, sets a minimum waterproofing design working life of 20 years for roof works.[3] The requirement concerns the roof waterproofing works. Ask a supplier claiming a 20-year design target to identify the full build-up, detailing, selection basis, inspection and maintenance conditions. A contractual warranty has its own period, terms and scope.

For comparison, Spanish assessment body IETcc evaluated two Neoproof Polyurea R roof systems under ETA 24/1247. Minimum thickness was 1.0 mm for the system without embedded reinforcement and 1.2 mm with embedded reinforcement. Both were assessed for an assumed working life of 25 years (W3) under the specified installation, service and maintenance conditions. The 25-year assessment applies only to the specified Neoproof Polyurea R systems and conditions. Claims about the service life or warranty of N300 or N700 require separate evidence.[4]

Read any working-life assessment together with the specific construction. Changing the reinforcement can change the specified thickness even with the same main coating. Available data do not establish four combinations of service life for N300 and N700 at 1.2 and 1.5 mm. For a claim that extra thickness adds years, ask for exposure records or an engineering assessment for that grade, thickness and system. Check the climate, observation period, failure criteria and repairs. Accelerated weathering hours cannot be converted directly into years on a roof.

Checking weathering reports before purchase

For N300 and N700, compare the full product name, colour, primer, substrate and specimen dry-film thickness. Then check the light source, irradiance, temperature, spray or condensation cycle, exposure duration and recorded endpoints. Two reports can both say “pass” while one measures only colour and the other also examines cracking and adhesion. For waterproofing, identify which relevant properties were measured before and after exposure, and which build-up the conclusion covers. Field records should describe the roof location, orientation, time in service and repairs.

If reducing future repairs is the objective, agree on what triggers intervention. Loss of gloss, local touch-up and roof leakage have different consequences and repair costs. Have the contractor identify inspection points, maintenance for drains, terminations and walkways, and the repair method for local damage. A defect that can be detected early and repaired locally has different cost implications. Include this when comparing the incremental material cost of greater thickness.

Budgeting for concrete, retained tiles and walkable terraces

On concrete, inspect soundness, dusting, cracks, old coatings and standing water. Remove or otherwise treat weak surface material and detail moving cracks and movement joints to the project specification. On rough or porous concrete, use a trial area to estimate levelling, sealing and absorption losses. Correct inadequate falls and high outlets and check drainage details before selecting a roof-field thickness.

Retaining tiles can be considered where the substrate is sound, clean and dry. Identify and address hollow or loose tiles, cracks and unstable grout. Prepare a representative adhesion trial over tile faces and joints with the proposed cleaning, surface preparation, primer and waterproofing layer. After the specified cure, check adhesion and the failure location using the agreed acceptance method. Widespread hollow areas, persistent moisture underneath or moving structural cracks require assessment of removal or repair first.

For regularly used terraces, assess wear, wet slip resistance and repairability. Itemise primary waterproofing, reinforced details and any wear-resistant, slip-resistant or protective finish. Confirm terminations at thresholds, parapets, pipe penetrations, floor drains and railing anchors. During application, record the mixing ratio, mass per coat, coverage and recoating conditions. Follow the grade TDS and site verification for mixing, recoating and curing. Check dry-film thickness, surface defects and detail continuity and perform the applicable waterproofing test.

How much material should a 100 m² quotation include?

For a net 100 m², 1.3 kg/m² gives 130 kg, or about 0.77 m²/kg. Assuming 1.6 kg/m² for budgeting gives 160 kg, or approximately 0.63 m²/kg. Verify on a trial area whether that application rate achieves the 1.5 mm target. The difference in the two budget quantities is 30 kg. Neither figure includes absorption, reinforced details, application loss or rounding up to pack size. Use representative trial consumption, field and vertical areas, terminations and pack sizes for the actual order.

Compare quotes on the same area and detailing basis. Check grade, combined A/B mass, target dry-film thickness, ancillary materials and acceptance method. A quote covering only the difference in main-coat quantity has a different scope from one including tile removal and repairs, drain terminations and a slip-resistant finish. Reconcile the work items before comparing prices.

Gaodun’s purchasing guidance

Prefer N300 for prolonged outdoor exposure. Consider N700 for standard weathering requirements. Both data sheets give a reference of 1.3 kg/m² for about 1.2 mm. A target of 1.5 mm and assumed consumption of 1.6 kg/m² are budgeting inputs pending technical confirmation; confirm the build-up by design and measure a representative trial area. If the design specifies 1.5 mm, use measured trial consumption to estimate the additional cost. Neither TDS quantifies a reduction in wear or a gain in service life from the added thickness. Where hollow areas, ponding, moving cracks or leaking terminations govern the risk, allow for those repairs first. Document the construction, approval basis, acceptance criteria and maintenance conditions for any specified project life.

References

[1] Covestro. *Pasquick® polyaspartic technology*. Technical brochure, pp. 18–19 (formulation chemistry and raw materials). The cited PDF gives no publication year. Source (solutions.covestro.com). Accessed 14 November 2026.

[2] Bratasyuk, N. A.; Latyshev, A. V.; Zuev, V. V. “Water in Epoxy Coatings: Basic Principles of Interaction with Polymer Matrix and the Influence on Coating Life Cycle.” *Coatings*, 2024, 14(1), 54. Section 2.1.1, equations (4)–(5). Source (doi.org). Accessed 14 November 2026.

[3] Ministry of Housing and Urban-Rural Development of the People’s Republic of China. *GB 55030-2022, General Code for Waterproofing of Building and Municipal Engineering*. 2022 edition, effective 1 April 2023. Clause 2.0.2. Source (mohurd.gov.cn). Accessed 14 November 2026.

[4] Instituto de Ciencias de la Construcción Eduardo Torroja (IETcc). *European Technical Assessment ETA 24/1247 — Neoproof Polyurea R*. First edition, 20 July 2025, English translation by the assessment body. Sections 1 and 2.2 and Annex 1. Source (dit.ietcc.csic.es). Accessed 14 November 2026.