POLYASPARTIC TECHNICAL ARTICLES
Polyaspartic Polyurea Technical ArticlesStorage Stability of Polyaspartic Polyurea: From In-Container Condition to Film Performance after Storage
To assess the storage stability of a two-component polyaspartic coating, check the packaging and storage conditions against the product data, inspect both components against the stated criteria, then prepare a test film at the specified mixing ratio by mass. Gaodun believes that storage stability should be evaluated throughout the synthesis, formulation, packaging and film formation of raw materials, with multiple batches of real-time samples and appropriate accelerated testing to jointly support product technical data. When checking the storage stability, verification of adhesion, flexibility, watertightness or clear topcoat appearance can be arranged according to the purpose, so as to facilitate the correspondence between the observation in the barrel and the film formation performance.
Article contents (9 sections)
1. Why is storage stability also part of material research and development capabilities?
From production to use, polyaspartic polyurea usually undergoes packaging, transportation, warehousing and on-site turnover. The fact that the material has qualified performance when it leaves the factory cannot alone prove that it will still have the same reaction and film formation performance after going through the above process.
The two-component system packages isocyanate and amine resin separately, which can avoid the major curing reaction between the two in advance, but it does not mean that each component will remain completely unchanged during storage.
Slow chemical changes may occur within the components, or crystallization, flocculation, sedimentation, or compatibility changes may occur. The degree of packaging sealing, temperature history and external moisture can affect these processes.
Gaodun believes that research and development needs to further extend "factory qualification" to "still meeting the use requirements within the specified storage conditions and period." This requires evaluating not just the state of the barrel, but also mixing, construction and final coating.
2. Shelf life, usage time after opening and mixed pot life. Why can’t they be mixed?
These three times describe different stages and rely on different evidence.
| concept | Corresponding status | Need clear conditions |
|---|---|---|
| Unopened shelf life | Part A and Part B are in specified packaging respectively. | Starting time, packaging, storage temperature and judgment indicators |
| Usable time after opening | The package has been opened, but A and B have not been mixed yet | Air contact, retrieval method, remaining volume and re-sealing conditions |
| Mix pot life | A and B have been mixed in proportion | Material temperature, mixing amount, environment and construction judgment |
| Durability time after film formation | The coating has been cured and ready for use | substrate, thickness, environmental and maintenance conditions |
Covestro Desmophen NH 1420 public information links the storage period to conditions such as original packaging sealing, moisture and heat protection and proper handling. The raw materials period cannot be directly used as the shelf life of Gaodun finished products.
Verification under unopened conditions cannot automatically cover repeated opening of the lid to take materials. After the package is opened, changes in air exchange, tool contamination, and remaining space within the container may occur.
Similarly, storage stability in barrels cannot be used to deduce the service life after film formation. The environment and mechanism of change between the two are different.
3. Part A has not gelled yet, why do we still need to check the NCO and viscosity?
Part A contains isocyanate group that can participate in curing. Even if obvious gel has not yet appeared, some degree of compositional change may have occurred.
After moisture enters, side reactions can occur with isocyanate, consuming NCO and producing carbon dioxide and related reaction products, thereby affecting viscosity, uniformity and subsequent film formation. Whether other slow reactions are significant needs to be judged based on the structure, catalyst residue and storage conditions.
Some Covestro polyisocyanate product information points out that the material is sensitive to moisture, and higher storage temperatures may lead to increased color and viscosity. This information illustrates the control direction, and the specific Gaodun Part A still needs to be independently verified.
The decrease in NCO and the increase in viscosity are not always synchronized. Just because the viscosity is close to the initial value does not mean that the reaction equivalent has not changed at all; nor can it be assumed that the original performance has been restored after the viscosity is adjusted back by adding diluent.
When a turbid or solidified appearance occurs at low temperatures, it is also necessary to distinguish between reversible physical changes and irreversible reactions. Without product verification, the heating recovery methods of other raw materials should not be directly applied to finished products.
4. Part B looks normal, why might it still affect the construction window?
When checking stored Part B, first identify the finished product model, component and batch number. Check appearance and the inspection items listed for that model. A Part B designation alone does not identify individual pigments, fillers or additives.
For resins, you can pay attention to the amine value, viscosity, chroma, moisture and necessary composition analysis; for pigmented and filler products, you also need to observe the settlement, redispersion, floating color and viscosity recovery.
If there are residual reactants in the system or slow reactions that can continue to occur, the reactivity may change after storage. However, this mechanism should be supported by analysis and mixing experiments, and a certain reaction cannot be determined based on changes in pot life alone.
The total amine values are similar and cannot completely represent the same distribution of different amine components. If the formula is sensitive to a small amount of highly active components, attention should also be paid to whether its changes affect the viscosity growth and surface dryness after mixing.
Gaodun believes that the stability of Part B should answer two questions: Can the barrel remain in a uniform and usable state? After mixing with specified Part A, is it still within the original construction and curing range?
Slight sedimentation that can be redispersed should not be directly regarded as scrapped; however, just because it can be stirred up, it cannot be assumed that the color, proportion uniformity and film formation performance have been restored.
5. Why can’t the number of days stored at high temperature be directly equal to the number of months stored at room temperature?
Raising the temperature can speed up some changes, helping to screen recipes faster. However, storage failure may simultaneously involve chemical reactions, particle settling, crystallization, solubility changes, and packaging compatibility, which do not necessarily have the same temperature dependence.
Some changes that are not dominant at normal temperatures may become dominant processes at excessively high temperatures. Conversely, low-temperature crystallization or transportation temperature cycling problems may not be exposed by constant high-temperature testing.
Therefore, "How many days at high temperature equals how many months at normal temperature" needs to be related to the data of the product itself and cannot be used as a universal conversion for all polyaspartic polyurea.
ASTM D1849-95 (2019) involves the packaging and storage stability of liquid coatings, focusing on consistency and other state changes. It provides an evaluation reference, but does not mean that the shelf life demonstration of reactive two-component products can be completed with just one storage test. ASTM D1849-95(2019) Official Summary (store.astm.org)。
A more reliable path is to parallel accelerated filtering with real-time storage. If a kinetic model is established, the applicable temperature zone, failure mechanism and prediction error should be verified, and then independent batches should be used to check the prediction effect.
6. How to include raw materials, packaging and sampling into the same verification plan?
The objects of the storage stability test should be as close as possible to the actual delivered products.
Small glass vials allow for easier viewing, but their seals, headspace, and contact materials may differ from commercial packaging. If the barrel, lining, gasket or packaging specifications are changed, the difference should be evaluated based on whether it affects the original conclusion.
To investigate a storage anomaly, record the package condition, visible leaks, batch number and storage temperature history. If before-and-after weights exist for the same package, compare them. A temperature change or a photograph of the container alone cannot establish internal pressure or the cause of the anomaly.
Sampling method is equally important. Opening the same container repeatedly will continually change the air exposure history. For unopened shelf life research, independent sealed samples can be set up and unsealed at planned time points; use separate samples and simulate the intended opening and withdrawal pattern when studying use after opening.
ISO 15528:2020 (iso.org) covers sampling of paints and their raw materials. ISO 1513 addresses subsequent sample preparation. For coatings containing pigments or extenders, the original settlement state should be recorded first, and then homogenized and sampled according to the prescribed method to avoid deviations caused by only extracting the upper liquid.
7. It can still solidify after storage. Why do we need to check the final coating?
The fact that the material can still form a solid does not fully indicate that the construction window, network structure and protective performance remain stable.
To assess application properties after storage, use the matched components of the specified finished product and prepare a sample at the mass ratio and conditions in its current TDS. At recorded time points, check the mixture for the intended application and document film formation on a test panel. A visual inspection of one component covers that component only.
The following control combinations can be set up during R&D to assist in identifying the source of changes:
| control combination | Main purpose |
|---|---|
| Baseline A + Baseline B | Establish a reference for this test |
| After saving A + base B | Observe the impact of changes in Part A |
| Base A+B after saving | Observe the impact of Part B changes |
| After saving A + After saving B | Evaluate the actual performance of the complete set |
The reference sample here needs to be confirmed, and the other set of retained samples cannot be assumed to remain unchanged forever. Sample batch variations should also be controlled or recorded.
The mixing test should unify the material temperature, proportion, mixing amount and operation method, and then observe the viscosity growth, pot life, surface dry, foaming and film formation appearance. When evaluating the final coating, the substrate, film thickness and curing conditions should be controlled.
Roofing materials can focus on adhesion, flexibility and watertightness; clear topcoat can focus on color, clarity and wear resistance; industrial protection can be combined with specific media and barrier requirements.
Not all long-term projects need to be completed at every point in time, but when the proposed deadline is approaching and abnormal trends occur, there should be sufficient film formation evidence to support the judgment.
8. How does Gaodun transform storage research into traceable product information?
Gaodun believes that the shelf life should respond to clear product model, packaging, condition and acceptance criteria, and be supported by representative multi-batch data.
R&D can pre-set acceptable ranges for appearance, viscosity, reaction indicators, construction windows and key film formation properties, and continuously record changing trends. A certain data is still within the limit, but it continues to approach the boundary, and it is also worth analyzing its subsequent risks.
Testing should also consider reproducibility. Whether the viscosity difference comes from temperature, shear history or instrument conditions needs to be distinguished first to avoid mistaking test fluctuations for material changes, and to avoid using fluctuations to cover up real drifts.
For materials that have exceeded the marked period, normal appearance is not enough to support continued use; re-inspection should not automatically lead to a unified extension of the shelf life. The manufacturer should make specific judgments based on batches, storage history and verification results.
After the formula, raw materials supplier or packaging is changed, whether the original storage data can continue to be applicable needs to be assessed based on the impact of the change. In this way, "detection traceability" can cover raw materials, production batches, packaging and subsequent use performance at the same time.
Facing subsequent technology development, Gaodun focuses on correlating composition analysis, rheological changes and film formation results, identifying earlier change signals, and using real-time retained samples to continuously verify judgments.
Gaodun believes that the storage stability of polyaspartic polyurea should be reflected in the material's ability to maintain predictable mixing reactions, repeatable construction performance, and film formation properties that meet the requirements under specified conditions and periods.
Further reading and technical information
The links below provide background on the topic. When it comes to specific performance, product selection or engineering parameters, please check the applicable objects and test conditions of each data.
- Covestro: Desmophen NH 1420raw materials technical specifications and storage requirements (solutions.covestro.com)
- Covestro: Pasquick polyaspartic ester technical data (solutions.covestro.com)
The above original data is used to verify the corresponding technical principles, research formulas or construction examples, and is not the testing or certification of Gaodun products. Research conclusions should be understood together with formulas, specimens and test conditions; construction parameters of products from different manufacturers cannot be directly interchanged.