POLYASPARTIC TECHNICAL ARTICLES

Polyaspartic Polyurea Technical Articles

Is Higher Polyaspartic Polyurea Adhesion Always Better? Comparing Test Values on Concrete, Tiles and Metal

The adhesion data of polyaspartic polyurea needs to be interpreted in combination with substrate, pre-processing, compatible coating system, curing conditions and damage location. Test results on concrete, ceramic tiles and steel plates cannot be directly ranked without conditions. Gaodun believes that long-term and solid protection should pay attention to the initial bonding, maintenance after the use of the environment, as well as the reliability of the on-site substrate and interlayers. When checking the report, the substrate, substrate processing, test status and damage location should also be recorded. If the damage occurs inside the substrate, the readings obtained cannot be directly regarded as the limit adhesion value of the coating and substrate interface. The results of different substrates should be read and compared separately. and check the specific levels at which the damage occurred.

Article contents (6 sections)

"This adhesion is 10MPa, and the other one is only 2MPa. Is the former five times better?" "The merchant pulled the coating from the cement board and still carried the cement. Can it prove that it will not fall off for a long time?"

Consumers are concerned about adhesion because roof waterproofing, tile renovation and metal corrosion protection all require coating to be firmly combined. However, only when an adhesion number is put back into specific testing conditions can we explain what conclusion it really supports.

For Gaodun, adhesion is not only a material research and development indicator, but also a performance that needs to be verified when moving from a laboratory compatible system to an actual substrate.

1. What exactly does the adhesion test measure? The numerical value and the damage location should be looked at together.

In a typical pull-off adhesion test, a loading fixture (dolly) is bonded to the coating surface with a test adhesive. A tensile load is applied perpendicular to the surface, and the pull-off stress is recorded under the specified conditions. The stress is reported in megapascals (MPa): 1 MPa equals 1 N/mm².

What is stressed during the inspection process is not only the interface between coating and substrate, but also the loading head, test glue, each layer of coating film and substrate.

ASTM D4541-22 is mainly used for metal substrate coating. The test-to-failure procedure records the pull-off results and section, and specifies the load procedure to check whether the specimen remains intact under the load. When the latter passes, it can only mean that the specimen has withstood the specified load. When comparing reports, you should check the procedure, substrate, instrument, adhesive, pull-off dolly size, curing and loading conditions, and identify whether the damage occurred in the adhesive layer, inside the coating, between layers or at the substrate interface. Concrete coating See also ASTM D7234.

Therefore, the report must not only look at "how much it is pulled", but also "where it is disconnected."

Table 1
main damage location How to understand
between coating and substrate Reflects the limitations of interface binding under this condition
between bottom layer and surface layer Need to pay attention to interlayer attachment and compatible system conditions
inside coating It needs to be combined with the analysis of the cohesive strength of the coating film itself.
Concrete and other substrate interior This damage is limited by the local strength of the substrate
Test the inside of the glue or its bonding points Judgment of target interface strength is limited by test glue

In actual sections, multiple types of damage may occur at the same time. The complete report should record the corresponding position and proportion, not just the highest value.

ASTM has also set up D7234 for the pull-off testing of coatings on concrete, and clearly emphasizes that both pull-off strength and failure mode are significant. This also reminds consumers that the detection method should be suitable for the substrate being tested.

2. Why can’t 2MPa on concrete and 10MPa on steel plate not be ranked directly?

Assume that the test results under two different conditions are: 2MPa on the concrete, the damage occurs inside the concrete; 10MPa on the steel plate, the damage occurs at the interface between the coating and the steel plate.

These pull-off adhesion values are hypothetical examples. The concrete specimen fails within the concrete at 2 MPa, so the limiting strength of the coating-to-concrete interface has not been measured. The other specimen fails at the coating-to-steel interface at 10 MPa. That value describes only the hypothetical steel specimen.

The above are only assumptions to explain the principle and do not represent Gaodun product testing data.

Take concrete coating as an example,ASTM D7234-22 Official Summary (store.astm.org)It shows that damage will occur on the weak side of the test combination. When reading the report, you should also check the measured value and the location of damage, such as inside the concrete, inside the coating, or at the interface between layers.

It is also important to note: Cohesive failure of concrete does not automatically mean that the site is qualified. If the substrate surface itself is weak, even if the interface is not separated first, the entire protection system may still be limited by the strength of the substrate.

When making judgments, you should also confirm whether the results meet the project requirements, whether the substrate is reliable, and whether the sampling location is representative. Neither the location of the damage can be ignored, nor can any lower value be considered acceptable simply by "bringing up the cement".

3. What are the different requirements for strong bonding between ceramic tiles, concrete and metal?

Different substrates have different surface states and potential weak layers, which cannot be summarized by just the same material name.

Concrete substrate, focusing on surface quality and water content.

Laitance, dust, surface dusting and oil will affect the surface that the coating actually comes into contact with. The higher strength of the concrete below does not mean that weak objects on the surface can be retained.

Tile substrate, focusing on surface adaptation and original paving stability.

Glaze, polished surfaces, wax or antifouling treatments will change the coating contact conditions. At the same time, the coating is well bonded with the tile surface, which does not prove that the adhesive layer on the back of the tile has no hollow-sounding areas or is loose.

Before retaining existing tiles, check for hollow or loose areas and contamination. Repair unsound areas, prepare a sound, clean, dry surface for the proposed system, and verify adhesion on a trial area.

Metal substrate, focusing on corrosion, pollution, surface treatment and original coating.

Just because the new coating is firmly adhered to the old paint, it does not mean that the old paint is equally reliable with the steel plate. If rust occurs or the original paint peels off, the new system may also fail.

Covestro steel structure corrosion protection information discusses the primer's role in substrate attachment and corrosion protection, the middle layer's role in shielding, and the surface layer's role in weather protection. This way of describing responsibilities by layer helps determine whether the entire compatible system covers actual needs. Covestro

Gaodun believes that substrate adaptation verification should be specific to the material surface and processing status. Excellent results on steel are not a direct substitute for judgment on suitability on ceramic tiles, old paint or surface dusting concrete.

4. It is very strong just after it is finished. Why should we pay attention to the maintenance after being exposed to water and sunlight?

The initial adhesion answer is to detect the binding performance at that time. During long-term use, roofs and terraces may also experience rainfall, local water accumulation, temperature changes and wear and tear, and metal surfaces may be subject to corrosion.

These factors will act on the coating film, interface and substrate. Only examining freshly cured specimens does not provide a comprehensive answer as to whether the bond will remain after years of use.

For practical purposes, Gaodun advocates further extending the verification to the state after the corresponding environment, for example:

  • How does the adhesion performance and damage location change after water resistance or moist heat treatment?
  • Whether cracking, blistering and interlayer separation occur after artificial aging or temperature cycling.
  • How does the metal corrosion protection compatible system change around the damaged area after the specified corrosion test?
  • Do actual exposure records show stability at edges, seams, and local repairs.

The processing conditions and evaluation methods here should be determined based on the specific use, and arbitrary soaking times cannot be used to establish general conclusions.

When comparing data before and after aging, you should also check the detection status: test immediately after treatment, or test after drying and recovery? If the method or state is different, numerical changes require further explanation.

The maintenance of adhesion has reference value, but it should still be evaluated together with waterproof continuity, mechanical properties and appearance changes, and cannot be converted into service life alone.

5. How can consumers obtain useful evidence of adhesion when purchasing?

Instead of just asking "how many MPa can it reach?", it is more effective to ask clearly what the data corresponds to.

First, what substrate is being tested?

Confirm the specific type of concrete, tile or metal, whether there is original coating, and what pre-treatment was used.

Second, are you testing a single layer or a complete compatible system?

Confirm whether it contains primer coat and surface layer, and whether the model and thickness of each layer are consistent with the purchase plan.

Third, what methods and conditions are used?

Understand the instrument, curing time, temperature and humidity, whether to cut, and whether the result is a single value or multi-point statistics.

Fourth, where does the damage occur?

Ask to see cross-section records, damage proportions and photos, and avoid looking at excerpted numbers.

Fifth, can the evidence correspond to the scene?

When conditions permit, conduct trial coating and verification of the compatible system in a representative area, and then evaluate according to project requirements. Pull-off adhesion testing can damage the coating. Plan for repairs at the test locations.

For R&D and production companies like Gaodun, the value of technology should be reflected in the matching of formula and substrate, compatible system verification and traceable delivery. When explaining adhesion to the outside world, the numbers, conditions and scope of application should be provided together.

What consumers want is for materials to remain strong in their substrate and usage environment. Being able to explain clearly "what was measured, how to destroy it, and whether it is applicable" can help transform adhesion data into reliable purchasing basis.

Further reading and technical information

The links below provide background on the topic. When it comes to specific performance, product selection or engineering parameters, please check the applicable objects and test conditions of each data.

The above original data is used to verify the corresponding technical principles, research formulas or construction examples, and is not the testing or certification of Gaodun products. Research conclusions should be understood together with formulas, specimens and test conditions; construction parameters of products from different manufacturers cannot be directly interchanged.