POLYASPARTIC TECHNICAL ARTICLES
Polyaspartic Polyurea Technical ArticlesCoordinated Pigment and Filler Design in Polyaspartic Polyurea: Why Can the Same Resin System Deliver Different Durability?
Even with the same resin, changing the pigment or filler changes the particle surfaces the resin must wet. Poor wetting, particle agglomerates or unfilled voids can leave weak areas at the resin–particle interface. To compare formulations, record pigment volume concentration (PVC) and dispersion, prepare panels on the same substrate at the same dry film thickness, and test durability under the intended exposure conditions.
Article contents (9 sections)
1. Why are pigments and fillers part of the material structure design?
When comparing two polyaspartic formulations made with the same resin, record the pigment and filler grades and their volumes. The binder must fill the spaces between particles. Examine each cured panel to assess film continuity.
Reasonable selection of pigments and fillers can achieve covering, color adjustment, rheology adjustment or specific enhancement, and may also improve barrier performance under certain conditions. But agglomeration, insufficient wetting, or overfilling can introduce weak areas.
Therefore, Gaodun believes that to evaluate a polyaspartic polyurea, one must not only understand the chemical structure of Part A and Part B, but also understand how pigments and fillers participate in the formation of the final coating.
"Using the same resin" provides the basis for the formula, and the specific performance of the finished product still needs to be verified separately.
2. Why does adding the same mass not mean that the particles occupy the same volume?
Formula production is usually based on mass input, but the volume occupied by the particles in the dry film is more directly related to its spatial distribution.
Different pigments and fillers have different densities. Two powders with the same mass may occupy significantly different volumes, and their structural impact cannot be judged just by "adding a few percent".
Pigment volume concentration, usually abbreviated as PVC, is referred to in this article as:
PVC = Pigment and filler volume ÷ (Pigment and filler volume + non-volatile film formation volume) × 100%.
The PSLC explanation of pigment volume concentration (pslc.ws) gives the volume fraction of pigments and extenders in the combined volume of those particles and the nonvolatile binder. For a two-component reactive coating, include the film-forming components of both Part A and Part B and state the basis for the volume calculation.
Pigment volume concentration (PVC) is the volume of pigments and extenders divided by their combined volume with the nonvolatile binder in the dry film, expressed as a percentage. Volume solids is the dry film volume obtained under specified conditions as a percentage of the mixed wet coating volume.
Gaodun advocates that when comparing alternative powders, mass, density, volume and their impact on construction viscosity should also be accounted for.
3. Can the critical pigment volume concentration be used as a general performance dividing line?
Critical pigment volume concentration, often referred to as CPVC, is used to describe the state in a specific particle system where the film formation can just meet the requirements for particle wetting and inter-particle gap filling.
Beyond this range, changes in porosity and structural continuity may significantly affect penetration, gloss, and other properties. pslc.ws
At the critical pigment volume concentration (CPVC), a formulation contains just enough binder to wet its particles and fill the spaces between them. Reassess that threshold when changing the powder.
Oil absorption can help compare the liquid requirements of powders, but it cannot replace the film formation evaluation of reactive coatings without verification.
Even if the formulation is below the estimated CPVC, weak points may occur due to local agglomeration, insufficient foam removal, or construction defects. Therefore, PVC and CPVC are suitable for auxiliary design, and ultimately still need to be combined with actual film formation and performance testing.
4. If the dispersion fineness is qualified, why may color and performance changes still occur?
Powder dispersion includes processes such as wetting, agglomerate deagglomeration and subsequent stabilization. Achieving a certain fineness at the end of production does not mean it will always be stable during storage, mixing and curing.
BYK's public information summarizes the role of wetting and dispersing additives as helping particles to be distributed finely and evenly and maintaining system stability.
To investigate uneven colour on a polyaspartic panel, record the appearance of the pigment paste, the mixed A/B coating and the cured panel separately. Compare dispersion if pigment flocculation is suspected. A photograph of the finished panel only shows the visible difference.
During research and development, fineness, color, viscosity, storage stability and film formation performance after mixing can be combined for judgment.
The more dispersants you add, the better. BYK's technical information points out that excessive additives may affect coating film properties such as hardness and water resistance.
Gaodun focuses on the stable dispersion of the reaction system and the resulting performance balance of the finished product.
5. Regarding the weather resistance of white coating, why do we need to pay attention to the specific brand of titanium dioxide?
Titanium dioxide can effectively scatter visible light, providing coverage and brightness for white coatings. But its function is not only for whitening.
Chemours' public information states that the particle size and surface composition of titanium dioxide will affect its performance. Different surface treatments are related to dispersion, powder resistance and outdoor durability. Ti-Pure™ TiO₂ by Chemours
For organic resin coatings, it is also necessary to control the possible photocatalytic effects of pigments. Pigments used for long-term outdoor protection should be verified based on the crystal form, coating and specific application, and cannot be simply judged as "all titanium dioxide".
This does not mean that the more titanium dioxide, the better the weather resistance. Increasing dosage will simultaneously change the PVC, rheology and particle interface, and its combined effect needs to be verified.
Gaodun believes that the weather resistance conclusions of white, gray and transparent products should be implemented in the corresponding formulas; the results of one color cannot unconditionally cover all colors.
6. Why might the moisture brought in by pigments and fillers affect curing and film formation?
Powder and color paste may bring in moisture. When a side reaction occurs between water and isocyanate, part of the NCO will be consumed and carbon dioxide may be produced, affecting the original reaction balance and bubbles control.
Borchers' public information lists moisture in pigments, fillers and solvents as one of the objects to be controlled in isocyanate-related coating raw materials. Borchers: A Milliken Brand
Applying this principle to polyaspartic polyurea should be combined with the actual moisture content, raw materials composition and process verification, and the additives or treatment methods of other systems cannot be directly copied.
The drying weight loss of raw materials is not necessarily equal to the moisture content, because it may contain other volatile components. The detection method needs to be adapted to the specific powder or color paste.
In addition to moisture, attention should also be paid to the active hydrogen component and additive compatibility in the color paste carrier. Adding color paste may change the degree of dilution and reaction equivalent, and needs to be verified according to the specified dosage.
7. When fillers increase hardness, why do they not necessarily improve protective properties at the same time?
A hardness reading applies to the filled polyaspartic panel tested under the stated conditions. Assess wear resistance using abrasion results for that formulation. For protective service, also check test records for the intended medium and exposure.
Flaky fillers, when properly dispersed and oriented, may extend the media penetration path; they may also form defects if agglomerated or insufficiently moistened. If the hard particles are not firmly bonded, they may leave pits after falling off during wear.
When comparing two filler loadings, record the powder volume fraction and mixed viscosity for each. Use the same substrate, dry film thickness and curing conditions. Record elongation and visible film defects separately before judging the effect of the change.
| Adjust direction | Possible effects | Should be verified simultaneously |
|---|---|---|
| Add covering pigment | Masking and color changes | Viscosity, dispersion, weather resistance and continuity |
| Introducing flake fillers | Barrier improvements under specific conditions | Orientation, porosity, adhesion and flexibility |
| Introduce hard particles | Enhancements under specific wear conditions | Particle bonding, post-grinding defects and appearance |
| Change particle size distribution | Accumulation and rheological changes | Settlement, wetting and construction foam removal |
| Adjust surface treatment | Improve compatibility or dispersion | Curing, storage and water properties |
These are studyable pathways of action, and specific effects should be demonstrated by corresponding formulation data.
8. Gaodun’s research and development direction: establishing a verification chain between resin, particles and finished products
Gaodun believes that the design of pigments and fillers should be advanced simultaneously with the structural design of Part A and Part B, and the changes in raw materials should be traced back to the final product.
During research and development, a verification chain of “powder grade and surface treatment—moisture and dispersion state—mixing curing behavior—coating film structure—performance maintenance” can be established.
When changing pigment suppliers, colorant carriers or filler gradations, the corresponding indicators should be reviewed based on the scope of impact. Initial color and viscosity are close and do not fully demonstrate equivalent long-term performance.
For roofs, attention should be paid to continuity, flexibility and adhesion after aging; for industrial protection, barrier and medium environments should be combined; for decorative floors, wear resistance, texture and appearance maintenance need to be evaluated at the same time.
Gaodun believes that the durability of polyaspartic polyurea comes from the synergy of the resin network, pigment-filler interface and film formation quality, and should be verified through the testing and application records of the corresponding finished products.
Further reading and technical information
The links below provide background on the topic. When it comes to specific performance, product selection or engineering parameters, please check the applicable objects and test conditions of each data.
The above original data is used to verify the corresponding technical principles, research formulas or construction examples, and is not the testing or certification of Gaodun products. Research conclusions should be understood together with formulas, specimens and test conditions; construction parameters of products from different manufacturers cannot be directly interchanged.