Polyaspartic Polyurea Technical ArticlesWhy Is Fully Aliphatic Polyaspartic Polyurea Suited to Long-Term Exposure? Evidence and Limits for Coastal Durability
The long-term protection foundation of aliphatic polyaspartic polyurea comes from the joint design of isocyanate structure, diamine-synthesized polyaspartic ester resin, prepolymer soft segment and curing network. This article combines BASF, Covestro, UBE, international papers and European technology assessments to demonstrate the value of 1.3-1.5 mm dry film in coastal waterproofing corrosion protection, distinguishing between raw materials basis, long-term application history and specific product life evidence. The article explains separately the raw materials structure, finished product inspection and external roofing system evaluation. This allows the reader to check which set of materials, which exposure environment and which maintenance conditions each life claim is made for. The external system evaluation is only used to illustrate the conditional verification path.
Article contents (10 sections)
1. The basis for long-term exposure should start with the two components of raw materials.
When consumers hear "fully aliphatic polyaspartic polyurea", what they want to know most is: why this material is suitable for sun and rain, and whether it is worth investing in long-term waterproof corrosion protection.
To answer this question, we need to establish evidence along the four links of raw materials, reaction, film formation and service. We cannot just list adjectives such as "weather resistance, wear resistance, high adhesion".
According to the component labels in this article and Gaodun, Part A refers to the isocyanate curing agent, and Part B refers to the polyaspartic ester resin component; the A and B labels of other companies may be opposite.
The route discussed in this article can be summarized as:
aliphatic or cycloaliphatic isocyanate curing agent reacts with polyaspartic ester resin synthesized with aliphatic or cycloaliphatic diamine as the skeleton to form a cross-linked network containing urea bonds.
The Covestro Pasquick manual describes aspartate as a secondary amine with sterically hindered characteristics and shows its reaction route with aliphatic polyisocyanates. [1]
This forms the basis for material identity and network design, but has yet to answer the question of how many years a given recipe will last. Next, you need to look at Part A, Part B and the final coating formed by the two.
2. Part A: What kind of weather resistance basis does aliphatic isocyanate provide?
The NCO group of the isocyanate is responsible for the reaction, and the molecular skeleton to which it is attached will also remain in the cured structure. Therefore, curing agents should not only compare their NCO content, but also their structural categories.
HDI belongs to aliphatic diisocyanate; IPDI and H12MDI belong to cycloaliphatic diisocyanate. A cycloaliphatic has a saturated ring structure, which is not equivalent to an aromatic structure with a benzene ring.
BASF's "Basonat HI 100 NG MB" technical information clearly states that this product is an HDI-based aliphatic isocyanurate, used for light-fast and weather-resistant two-component polyurethane coating. [2] Covestro's IPDI cross-linker data also links corresponding cycloaliphatic products to lightfast, high hardness and weather-resistant applications. [3]
Gaodun technical judgment: These two types of official data support aliphatic and cycloaliphatic isocyanate as the design basis of raw materials for exposed coatings, but their performance in polyurethane applications cannot be directly used as finished product indicators of Gaodun polyaspartic polyurea.
From the perspective of structural selection, the use of these skeletons can avoid introducing typical aromatic isocyanate source structures into the declared film formation route. This is a design measure to control the risk of photochromism and does not mean that any photo-oxidation will not occur in the coating.
It should also be noted that trimers and prepolymers describe another dimension. Trimers can provide multifunctional connections; prepolymers can introduce different segments. Both may use aliphatic raw materials, and both need to check the actual composition.
Therefore, consumers should ask "what is the structure of the curing agent and how is it modified?" rather than just "is it a trimer" or "is it a prepolymer".
3. Part B: How does aliphatic diamine become polyaspartic ester resin?
"Using aliphatic diamine" requires further explanation of the synthetic route.
In a typical route, the Michael addition of an aliphatic or cycloaliphatic primary diamine to a dialkyl maleate produces a polyaspartic ester with a secondary amine reaction site. It is different from the starting primary diamine. "The original diamine reacts directly with the isocyanate" cannot be confused with "the polyaspartic ester resin is first synthesized and then cured".
In a paper published by Gheybi et al. in 2026, polyaspartic ester resin was prepared using isophorone diamine IPDA and diethyl maleate DEM, and the synthetic material was characterized. [4] This is a specific research example of cycloaliphatic diamine participating in the synthesis of polyaspartic ester resin.
This article only cites the synthesis and characterization route, and does not cite the performance data of the composite coating, nor does it use it as proof of long-term roof life.
The Covestro manual also states that the choice of polyaspartic ester resin skeleton will affect its reactivity with polyisocyanates and can be used to adjust pot life and drying time. [1]
Gaodun technical judgment: The value of Part B includes retaining the selected non-aromatic diamine skeleton and regulating the reaction through the secondary amine structure so that the material can be mixed, spread and cured within the appropriate construction window.
However, response adjustment does not mean automatically obtaining low defect coating. Excessive reaction may affect spreading and foaming, while insufficient reaction may leave areas that are not fully cured. The formulation and construction still need to be controlled together.
Part B cannot be judged to be fully aliphatic just based on the name "polyaspartic". The diamine source skeleton, other reaction resins and compounding conditions should be checked; for unverified commercial resins, the exact diamine composition should not be specified without authorization.
4. Why must Part A and Part B be explained at the same time?
After the two components are solidified, the skeleton of raw materials enters the network together. Therefore, just stating that Part A is aliphatic cannot replace the verification of Part B and other film formation components.
| raw materials or structural issues | Implications for long-term exposure judgments | What needs to be verified |
|---|---|---|
| Part A isocyanate backbone | Determine the structural origin of a partially solidified network | Does it contain aromatic isocyanate and its derivative components? |
| Part B diamine source skeleton | Determine part of the structure of polyaspartic ester resin | Whether a diamine synthesis route consistent with the statement is used |
| Prepolymer soft segment | Affects deformability and environmental stability | Polyol type, modification method and performance maintenance |
| Other film formation resins | May change the performance of the entire network | Is the compounding explained accurately and re-verified? |
| Pigments and stabilizing systems | Affects color, shading and aging performance | Whether transparent, white, and gray are verified separately |
| Curing status and defects | Determine whether the design can be converted into effective coating | Are proportioning, mixing, curing and continuity qualified? |
The discussion of "fully aliphatic" here refers to the host film formation structure within the clearly stated scope, and is not equivalent to requiring that every additive and pigment does not contain any aromatic rings. Enterprises should explain the caliber, and this article does not set a unified purity threshold.
Likewise, aliphatic and aromatic compounds may be designed for specific uses and costs; the key is to be truthful and not advertise them as being identical to fully aliphatic formulations.
The judgment that is easy for consumers to understand is that the two components jointly determine the structure of the film. Only half of the raw materials are explained, which cannot prove the entire formula.
5. The third layer of raw materials that is easily overlooked: prepolymer soft segment
Even if both isocyanate and diamine adopt an aliphatic or cycloaliphatic structure, the long-term performance of the product may still be different because polyether, polyester or polycarbonate segments may also be present in the prepolymer.
These segments can be used to adjust flexibility, modulus, and deformability, while also affecting stability under water, heat, and light.
UBE Europe's official technical description points out that its polycarbonate diol route has design advantages in hydrolysis resistance, heat resistance and UV degradation resistance in the corresponding polyurethane, and explains the difference between the carbonate group and common ester and ether structures. [5]
This is a supplier's technical description of their material route, and it cannot be directly concluded that all polycarbonate-containing formulations are superior to others.
Gaodun technical judgment: The prepolymer needs to be designed at the same time "whether it can withstand deformation" and "whether it can continue to withstand after aging", and cannot only be evaluated by initial elongation.
If the formula uses a combination of polycarbonate and polyether, its rigid-flexible balance and performance maintenance can be studied, but whether the specific ratio is reasonable should be confirmed by compatibility, mechanical and environmental tests.
Polyaspartic ester resin itself also contains ester groups. The aliphatic structure does not mean that all chemical bonds are not affected by water and the environment; the position of the ester group, network structure and contact medium are still important.
Therefore, "raw materials double aliphatic" is an important structural basis, but it is not a reason to omit water, heat and aging evaluation.
6. From the advantages of raw materials to waterproof corrosion protection, what kind of network needs to be formed?
The secondary amine in polyaspartic ester resin reacts with the isocyanate NCO group to form a urea bond; with the participation of multifunctional components, a cross-linked network can be formed. [1]
Gaodun technical judgment: Reasonable network design requires a balance between connection strength, link segment activity and defect control.
Insufficient network constraints may result in insufficient load-bearing, swelling, or continuous deformation; too strong constraints may also limit deformation capabilities, making the coating more likely to be damaged when the substrate changes repeatedly. The specific trend is affected by the formula and cannot be concluded based on "the denser the cross-linking".
For coastal waterproofing corrosion protection, what is valuable is a complete and stable barrier: one that can limit the transmission of moisture and ions while remaining continuous under temperature differences, substrate changes and local loads.
The formation and interaction of urea bonds provide a structural basis for material load-bearing, but it does not make the coating absolutely non-absorbent and impermeable. Water absorption, penetration, adhesion and defect expansion need to be evaluated separately.
Likewise, when using prepolymers, urethane linkage may coexist with subsequently formed urea bonds. Just because urethane linkage is detected, we cannot deny that polyaspartic ester resin is involved in the reaction; nor can we confirm the identity of all resins just because we detect urea linkage.
7. How does 1.3-1.5 mm dry film work?
The 1.3-1.5 mm in this article refers to the effective dry film thickness after curing. When evaluating, it should be clear whether it includes primer coat or other compatible system layers.
In a complete, uniform coating with the same performance, increased thickness can improve transmission resistance and provide a certain margin for mechanical damage. This is a judgment made by Gaodun based on the relationship between barriers and geometry, not a lifespan conversion model.
Thicker coatings will not automatically resolve pinholes, uneven mixing and debonding. Local defects may become preferential channels, and rough peaks, corners, and details may be thinner than the main surface.
Therefore, when evaluating the 1.3-1.5 mm plan, it is necessary to confirm at the same time: the raw materials route is correct, the curing is sufficient, the film thickness is reasonably distributed, the coating is continuous, and the interface is reliable.
Different substrates have different concerns:
| Application | Main protection tasks | Additional verification required |
|---|---|---|
| Concrete roofs and terraces | Waterproof and adaptable to substrate changes | Waterproofing, adhesion, cracks and cyclic deformation after aging |
| Coastal steel structures exposed to the atmosphere | Inhibits corrosion and keeps coating intact | Surface treatment, salt, primer coat, corners and damage spreading |
| Frequent traffic area | Waterproof and suitable for mechanical use | Wear, impact, anti-slip and inter-layer coordination |
| Splash or long-term seawater immersion | Protection under the continuous action of specific media | Special environmental assessment cannot follow the conclusion of ordinary roofing |
The raw materials structure provides the direction, the dry film thickness implements the barrier, and the complete system determines the application results.
8. Can these raw materials support a life span of more than 20 years?
Answers should be divided into three levels.
The first level is structural rationality.
aliphatic isocyanate, a suitable diamine source polyaspartic ester resin, and selected prepolymer segments provide an interpretable design basis for long-term exposure, but a 20-year value cannot be given individually.
The second level is the international application background.
Covestro officially states that Pasquick technology has more than 20 years of field application performance. [6] This is a corporate technology history statement, and this article does not obtain the project-by-project formula, film thickness and maintenance files behind it.
The third level is system-specific assessment.
IETcc-CSIC's ETA 24/1247 gives W3, 25 years expected working life for Neoproof Polyurea R specific roofing kits. According to Section 2.2 and Appendix 1, the minimum film thickness of System 1 without internal reinforcement mesh is 1.0 mm, and the minimum film thickness of System 2 with internal reinforcement mesh is 1.2 mm. Using this assessment also requires checking the substrate, compatible system, usage loads, and installation and maintenance conditions. [7]
This evaluation is not Gaodun product certification and is not sufficient to confirm that the external formula is the same as the Gaodun fully aliphatic formula. The EOTA document also makes clear that expected operating life cannot be interpreted as a guarantee. [8]
Gaodun technical judgment: Raw materials basis, international application history and specific system evaluation jointly support that "this is a technical route with a long-term protection foundation"; to implement the conclusion into Gaodun's 1.3-1.5 mm coastal solution, the company's corresponding finished product and system evidence are also needed.
Q-Lab explains that there is no universal conversion factor between accelerated aging hours and outdoor years. [9] You cannot add the advantages of raw materials to a certain aging hour and write it as a proven 20-year lifespan.
9. How to turn technical evidence into purchase reasons that consumers can verify?
Consumers don’t need to have the full recipe, but they can ask to verify five things.
First, the identity is clear. What is the structure of Part A, what resin route is used in Part B, and whether there are any compounds that affect the "fully aliphatic" statement.
Second, model correspondence. raw materials information, finished product model, color and production batch can be connected, but the supplier's material advantages cannot be directly rewritten into Gaodun test results.
Third, it still has functions after aging. In addition to observing discoloration and chalking, you should also observe the maintenance of waterproofing, adhesion, mechanics and corresponding corrosion protection indicators.
Fourth, film thickness can be accepted for inspection. 1.3-1.5 mm should become a quality control condition in a verified plan, not just a construction slogan.
Fifth, long-term cost transparency. Only when the conditions for inspection, partial repair and recoating are clearly explained can the full-cycle investment be compared.
For metal corrosion protection, PPG official information also distinguishes between compatible systems: KWIKSPAR polyaspartic coating uses designated epoxy primer in high-corrosion environments, and only introduces the alternative of direct metal coating in low-to-moderate corrosion environments. [10] This shows that excellent surface raw materials still need to correspond to the environment and underlying design.
Gaodun advocates that the long-term value of aliphatic polyaspartic polyurea should be explained from the two-component raw materials to the actual coating: why these structures are chosen, how to form the network, what properties are maintained after aging, and how to accept inspection and maintenance of the project.
What consumers deserve to buy are materials and solutions that can demonstrate and verify long-term protection capabilities. The fully aliphatic structure is an important piece of evidence, and complete delivery requires the other links to be established together.
References
[1] Covestro (Covestro): "Pasquick® polyaspartic technology. Change the coatings game.", official website technical manual version, unverified publication year, see "Polyaspartics chemistry – and our portfolio".Specific Source (solutions.covestro.com). Access date: 2026-11-01.
[2] BASF (BASF): "Basonat® HI 100 NG MB — Technical Data Sheet", July 2023 edition.Official technical information (download.basf.com). Access date: 2026-11-01.
[3] Covestro (Covestro): "A more sustainable IPDI-based crosslinker portfolio", official website article path in 2024, no clear release date found on the webpage.Specific Source (solutions.covestro.com). Access date: 2026-11-01.
[4] Mirreza Gheybi, Abdolreza Mirmohseni, Ali Olad: "Multifunctional fast-curing polyaspartic ester polyurea/PANI-CsC@TiO2 composite coatings with antistatic and anticorrosion properties", Scientific Reports, 2026, 16: 3648. The resin synthesis and characterization routes in the text have been verified.DOI and Source (doi.org);Open full text read (pmc.ncbi.nlm.nih.gov). Access date: 2026-11-01.
[5] UBE Corporation Europe: "ETERNACOLL® polycarbonate diol — Maximizing the performance and the durability of your polyurethanes over time", official website technical description, no version date marked.Specific Source (ube.es). Access date: 2026-11-01.
[6] Covestro (Covestro): "Heavy-duty corrosion protection coatings for steel", official website article path in 2026, no clear release date is found on the web page, please refer to the Pasquick FAQ section.Specific Source (solutions.covestro.com). Access date: 2026-11-01.
[7] Instituto de Ciencias de la Construcción Eduardo Torroja (IETcc-CSIC): "European Technical Assessment ETA 24/1247 — Neoproof Polyurea R", 2025-07-20, version 1, English translation, see Section 2.2 and Appendix 1.Evaluation documentSource (dit.ietcc.csic.es). Access date: 2026-11-01.
[8] European Organization for Technology Assessment (EOTA): "EAD 030350-00-0402 — Liquid Applied Roof Waterproofing Kits", August 2018 version, published document in 2020, see Section 1.2.2 and Appendix 1.official assessment document (eota.eu). Access date: 2026-11-01.
[9] Q-Lab Corporation: "LU-0833 Correlation Questions & Answers", 2025 updated version.Specific Source (q-lab.com). Access date: 2026-11-01.
[10] PPG: "PPG introduces KWIKSPAR 600 and 600SG coatings for faster return-to-service", 2017, official technical release information.Specific Source (news.ppg.com). Access date: 2026-11-01.