POLYASPARTIC TECHNICAL ARTICLES

Polyaspartic Polyurea Technical Articles

Evaluating Industrial Corrosion Protection with Polyaspartic Polyurea: How Do Salt Spray Hours Support Evidence for a Complete System?

When polyaspartic polyurea is used for industrial metal protection, the salt spray test can provide relative corrosion resistance information under specified conditions, but it cannot determine the actual service life alone. Gaodun combines open standards and international industry data to discuss the relationship between a complete compatible coating system, scratch corrosion expansion, cyclic corrosion, wet adhesion and engineering tracking, and explains how to establish a corrosion protection evaluation for specific environments. Polyaspartic polyurea can be used for industrial metal surface protection. When evaluating its corrosion resistance, salt spray test is a common method, but the number of hours must be understood in conjunction with the sample structure and judgment indicators.

Article contents (9 sections)

1. What information does the salt spray test provide?

Polyaspartic polyurea can be used for industrial metal surface protection. When evaluating its corrosion resistance, salt spray test is a common method, but the number of hours must be understood in conjunction with the sample structure and judgment indicators.

ASTM B117-26a specifies salt spray equipment, test procedures, and controlled environments. The sample type, exposure time and result interpretation of specific products need to be checked in the corresponding specifications or project documents. Extrapolation of performance to natural environments should be supported by appropriate long-term atmospheric exposure data.

Therefore, "salt spray 2000 hours" requires further explanation:

  • substrate and surface treatment status.
  • Primer, main coat and top coat compatible system.
  • Actual dry film thickness of each layer.
  • Whether there are scratches and how to seal the edges.
  • Evaluation results of rust, blistering, corrosion expansion and adhesion.

Gaodun believes that the number of hours belongs to the test record, and only complete information can support the judgment of corrosion protection.

2. Why should corrosion resistance belong to the specific coating system?

Metal corrosion protection usually consists of substrate treatment, bottom layer, shielding layer and surface layer. Each layer can assume different functions such as adhesion, barrier, corrosion inhibition or weather resistance, depending on the formulation.

ISO 12944-6:2018 stipulates laboratory evaluation methods for carbon steel structure protective coating systems, and clarifies that the test is used to assist in selecting a suitable system, and does not provide precise durability years. Part 6: Laboratory performance test methods

The results obtained when a certain surface layer is used on mature primer cannot be directly described as the results of that surface layer on bare steel. Similarly, the performance of bare steel test panels cannot replace the interlayer verification of all compatible system combinations.

Gaodun advocates that the corrosion protection conclusion should be corresponding to the specific substrate, primer, main coating, surface layer and film thickness to avoid mistaking the system results for the inherent performance of a single raw material or single layer of coating.

3. Why do intact test panels and scratched test panels need to be evaluated separately?

The complete test panel is mainly used to observe the shielding and stable performance of continuous coating in the specified environment. The scratch test plate exposes the metal through prescribed damage to study the corrosion and coating peeling expansion near the defect.

Corrosion of exposed metal at scratches does not mean that the entire system has failed to the same extent. The evaluation also focuses on whether the damage extends to both sides and whether the surrounding coating can maintain union.

Table 1
Observation content Main answer
Complete area rusting, blistering Whether the coating film body and local defects have become weak links
Expansion of corrosion or peeling around scratches Can corrosion and interface separation expansion be limited after damage?
Damage near edges and welds Do geometric positions and coverage affect performance?
Attachment after test How does binding performance change after environmental effects?
Film cracks and interlayer separation Is system integrity maintained?

The shape, width, depth and cleaning evaluation procedures of scratches need to be clearly defined. Data without scratches and scratches cannot be ranked indiscriminately.

4. The value of cyclic corrosion lies in the targeted environmental path

Continuous salt spray provides a controlled environment, but actual components may also experience drying, condensation, temperature differences and sunlight.

From the analysis of corrosion mechanism, changes in dryness and humidity will affect salt concentration, water film state, oxygen supply and coating absorption and dehydration; it is not simply equivalent to continuous moisture.

Loop experiments can organize these effects around the target environment, but just because there are more steps or harsher conditions should not be considered more accurate.

Gaodun recommends identifying the application type first:

  • Coastal atmospheric exposure.
  • Long-term soaking.
  • Splashing and repeated wetting and drying.
  • Industrial chemical media.
  • Environments accompanied by mechanical wear or impact.

Then choose the applicable method accordingly. Results from different environments cannot be compared based solely on hours of exposure, nor should one general cycle program cover all industrial applications.

5. Wet adhesion and electrochemical tracking to supplement the deficiencies in appearance observation

When there is no obvious rust on the coating surface, medium entry and interface changes may still have begun. Gaodun recommends combining appearance, wet adhesion and applicable electrochemical methods for phased tracking.

Wet adhesion requires clear sampling, bonding and pulling heads and testing procedures to avoid drying and recovery from changing the state under study. Electrochemical impedance requires control of film thickness, area, electrolyte, temperature and frequency.

The high impedance at a single point in time cannot directly determine the multi-year life; the adhesion value after the test should also be combined with the damage surface analysis.

Different methods jointly point to a certain change, which is usually more explanatory than isolated results.

For engineering applications, attention should also be paid to edges, connections and repair locations so that standard test panels complement the actual components.

6. International industry direction: reducing the number of coating passes requires complete verification

Covestro's 2026 public information introduces Pasquick®polyaspartic polyurea corrosion protection technology and discusses the design route of a two-layer compatible system and direct metal coating. Covestro

This reflects the industry direction of improving coating efficiency through high solids, rapid curing and formula synergy. However, it cannot be deduced from this that the primer can be omitted for all polyaspartic polyurea, nor can the verification results of the supplier's specific formula be transferred to other products.

Reducing the number of passes still requires meeting the requirements for total dry film thickness, partial coverage, interlayer bonding, and target environmental protection.

Direct coating of metal (DTM) does not mean that oil removal, rust, oxide layer, salt and surface condition can be ignored.

Gaodun believes that channel number optimization should be based on a complete solution that is producible, constructable and verifiable.

7. How to form traceable evidence of industrial corrosion protection?

The following are R&D evaluation suggestions, and specific tests and criteria should be determined according to application requirements.

  • Clarify environment, substrate and maintenance goals.
  • Fixed compatible system composition and dry film thickness of each layer.
  • Record surface treatment, batch, curing and overcoating conditions.
  • Set complete area, scratch and edge evaluation by method.
  • Set up replicates and controls of known performance.
  • Record changes in appearance, erosion, and adhesion at inspection points.
  • Link laboratory results with on-site tracking of corresponding components.

Photographs should retain scale, orientation, specimen number and time. For scratch expansion and corrosion, the measurement and calculation methods should also be explained to avoid direct comparison of the results of different calibers.

Batch comparisons should try to control sample preparation and equipment differences; engineering results need to record repairs, maintenance and abnormal environmental events.

8. Gaodun’s technical stance: transforming material advantages into environmentally adapted protection solutions

Shenzhen Gaodun New Materials Co., Ltd. has focused on polyaspartic polyurea systems since 2016, focusing on the research and development, synthesis, formulation and production of Part A and Part B.

Gaodun believes that the research and development of industrial corrosion protection should integrate resin and curing agent design, pigments and fillers, substrate treatment and compatible system as a whole to match rapid curing and long-term protection.

For applications such as steel structures, carriages, and equipment shells, the environment, mechanical damage, film thickness, and maintenance conditions should be clarified respectively, and evaluations should be established through corresponding systems.

This article is a technical analysis and R&D evaluation suggestion. It does not mean that Gaodun has completed all the tests in the article or obtained relevant environmental grade certification. Specific model performance, substrate and compatible system requirements are subject to the corresponding technical instructions, test reports and engineering plans.

Further reading and technical information

The links below provide background on the topic. When it comes to specific performance, product selection or engineering parameters, please check the applicable objects and test conditions of each data.

The above original data is used to verify the corresponding technical principles, research formulas or construction examples, and is not the testing or certification of Gaodun products. Research conclusions should be understood together with formulas, specimens and test conditions; construction parameters of products from different manufacturers cannot be directly interchanged.