Polyaspartic Polyurea Technical ArticlesCan Polyaspartic Polyurea Be Thinned? Does More Thinner Save Material or Leave the Waterproofing Layer Too Thin?
Polyaspartic polyurea feels a bit thick, can I add diluent? Is it more cost-effective to brush more easily after adding it and cover a larger area? Gaodun believes that whether dilution is allowed should be determined by the specific model, construction method and process. Lowering the viscosity can improve certain construction conditions, but ordinary volatile diluents will not increase the effective film formation material. This article combines the technical data of Covestro, Asahi Kasei and other companies to explain the relationship between constructability, solids content and final thickness from five directions. Compare thinning options over the same area at the specified dry film thickness. Record coating and thinner consumption, number of coats, labour, waste and inspection costs.
Article contents (6 sections)
1. Where does low viscosity come from: Material design and on-site solvent addition are not the same thing
The paint flows easily, which may be due to the low viscosity of the resin and curing agent itself, or because the formula contains volatile solvents. Both cases look "thin", but the actual basis of film formation is different.
Covestro's high solids technical information points out that the low viscosity of the polyaspartic ester binder is conducive to the design of ultra-high solids and even near-zero VOC coatings. This shows that good workability does not have to rely entirely on adding a large amount of solvent on site. Covestro
Asahi Kasei's low-viscosity DURANATE™ data also introduces solvent-free, high solids low-viscosity curing agent grades; its polyaspartic ester application data further discusses the impact of low-viscosity compatible systems on operability.
To compare viscosity results, identify the product and component, test method and test temperature. For the measured value of a particular batch, consult its batch test record.
Gaodun believes that it is more meaningful to check the original solid content, specified construction status and corresponding performance of the product. Manufacturers achieve low viscosity through raw materials and formula design, and construction workers temporarily add unknown solvents, which cannot be regarded as the same technical route.
2. When can it be added: It must correspond to the model, process and system documentations
There is no uniform dilution ratio for polyaspartic polyurea that applies to all products.
Some models can be constructed after mixing according to the original ratio; other systems may allow the addition of specified diluents in specific processes. For example, a proven concrete penetration primer may have different construction status requirements than forming a main surface waterproofing layer of specified thickness.
For the first penetrating sealing coat on a Gaodun concrete roof, add the specified compatible thinner at 20%–30% of the total weight of mixed Parts A and B. For example, when 10 kg of Parts A and B has been weighed at the specified product ratio, add 2-3 kg of thinner; the resulting total weight is 12-13 kg. First confirm the A/B ratio and measurement method on the supply label, then calculate thinner separately. For the second and third coats, prepare a fresh batch at the ratio specified for the selected product, without adding extra thinner. Existing tiled terraces follow the tile-substrate procedure.
For processes that allow dilution, Gaodun advocates stating at least four things: what to add, how much to add, which calculation basis is used, and which process it is used for.
| What needs to be confirmed | Why is it important |
|---|---|
| Specific model of diluent | Different products have different compatibility and evaporation characteristics |
| Allowable addition amount | Involving leveling, curing and effective film formation |
| weight ratio or volume ratio | The two ratios cannot be mixed directly. |
| Calculate base | Calculation based on Group A, Group B or mixed materials, the results are different |
| Process usage | The conditions for priming, rolling or spraying cannot be copied at will. |
| Adjusted dosage and curing | Don’t just focus on ease of construction without looking at the final result |
Adding diluent does not replace the specified ratio of Part A and Part B. Even if a process allows the addition of additional compatible system solvents, it does not mean that one of the reaction components can be reduced or increased.
Water, alcohol, general-purpose "Tina Water" or tool cleaners are not suitable by default just because they reduce viscosity. The materials used to clean tools may have different requirements than the materials allowed to be mixed into paint.
For systems containing isocyanates, there is also a need to control undue moisture or reactive impurities. Consumers should ask for corresponding instructions instead of trying out the paint themselves based on their experience with other paints.
3. Why thinning may increase coverage without reducing cost: effective film formation matters
Ordinary volatile diluents are mainly used to adjust the construction status and cannot directly increase the final dry film according to the added volume.
If more solvent is added to the same original paint and spread over a larger main surface area, the original paint and effective film formation material obtained per square meter will be reduced. Just because the surface is temporarily wet does not mean that the thickness will meet the requirements after curing.
This can be understood with a volume example just to explain the principle:
Assuming that 1 liter of mixed paint has a volumetric solids content of 90%, its theoretical non-volatile volume is 0.9 liters. After adding 0.2 liters of completely volatilized solvent and adding them approximately by volume, the theoretical volume solid content is about 75%, and the non-volatile volume is still 0.9 liters. Here is an instructional example of calculation by volume. The 20%–30% of Gaodun concrete’s first substrate sealing is measured by the total weight of A and B mixtures, and the two calculation bases should be checked separately.
This example is not a Gaodun product parameter, nor does it include construction loss and curing volume change. It explains: The increase in total liquid volume does not equal the increase in dry film material.
Under applicable calculation conditions, the theoretical dry film thickness can be estimated from the ratio of wet film thickness to volume solid content. Therefore, if you still only apply the same wet film thickness after dilution, the dry film thickness will usually decrease; if you want to maintain the target dry film, the application amount and process need to be adjusted accordingly.
A distinction should also be made between mass solid content and volume solid content. A certain solid percentage on the label cannot be used directly for film thickness calculations if the caliber is not stated.
What is really worth comparing is how much original paint is needed to achieve the design thickness, not how much main surface area each barrel can spread after dilution.
4. What is the difference between reactive dilution and ordinary solvents: they cannot be left to the site for replacement at will.
In materials research and development, there are also methods of adjusting the system through low-viscosity reactive raw materials. Certain components can participate in the film formation reaction, unlike ordinary solvents which mainly evaporate away.
The Covestro Pasquick® technical manual lists reactive diluents for use in high solids formulations. This is a formulation design tool and does not mean that consumers can purchase an "active diluent" and add it on site.
Reactive components may change reaction equivalent, cross-linked structure, operating time, hardness and flexibility. After addition, the ratio and finished product performance need to be re-evaluated. Even if the solid content is not significantly reduced, it cannot be inferred that the performance will remain unchanged.
Before thinning, check the TDS for the exact model. Confirm the permitted thinner, the coat in which it may be used, and whether the percentage refers to one component or to the mixed coating. Ask the supplier to clarify any missing information before adding thinner.
Gaodun believes that viscosity reduction at the formulation end and allowable dilution at the construction end should be managed separately. The R&D and production enterprise is responsible for determining the verified material combination, and the on-site execution is carried out in accordance with the corresponding documents.
Consumers only need to confirm one thing: whether the manufacturer clearly allows this model and process to use this material and proportion. When there is no clear basis, adding yourself should not be used as the default action.
5. What to do if the material becomes thicker: first check the cause, then compare the costs
The thickening of the material may be due to low temperature, the reaction may have advanced after mixing, or the storage state may be abnormal. Different reasons cannot be dealt with in the same way.
Due to the increase in viscosity caused by low temperature, the materials and construction temperature should be managed according to the document requirements; if the mixture thickens due to reaction, it cannot be assumed that the original operating time can be regained by adding solvent.
The reaction may still continue, and the material may appear to have returned to flow, but this does not mean that its film formation state and properties have returned to when they were first mixed. Therefore, it is not advisable to repeatedly dilute a mixture that has thickened, stringed, or started to gel.
Before opening the barrel, you can estimate the amount of construction that can be completed in a single batch based on personnel, tools and area, and arrange the ingredients in batches according to the model of pot life.
Before purchasing and construction, you can check the following:
| FAQ | Basis to be obtained |
|---|---|
| Raw materials are thicker, is this normal? | Description of corresponding temperature, model and status |
| Will adding thinner save money? | Original paint consumption under the same dry film thickness |
| Can I continue to use the dilution amount of primer? | Independent process requirements for the main waterproof layer |
| Does it still comply with the promotional data after adding it? | Verification scope corresponding to construction status |
| How to confirm that it is not thinned? | Dosage, actual area and thickness inspection |
| Can the leftover mixture be saved until tomorrow? | Count pot life from mixing, at the temperature and under the conditions specified for this product. Stop application if the pot life has expired or you cannot verify that the material is still within its specified conditions of use. Appearance alone cannot establish usability. Handle surplus material as directed in the product instructions. |
Compare thinning options over the same area at the specified dry film thickness. Record coating and thinner consumption, number of coats, labour, waste and inspection costs.
From Gaodun's R&D and production standpoint, improving workability should prioritize the collaborative design of resin, curing agent and formula, and provide a clear basis for necessary on-site adjustments. All construction problems cannot be left to the customer to solve with additional solvents.
Whether polyaspartic polyurea can be diluted should be determined by the corresponding product process. Easier brushing is only valuable if it maintains the required amount of film formation and performance. Increased coverage does not in itself prove to be more material-saving or more durable.
Note: The specific dilution method is based on the corresponding product and compatible thinner files. International company information is used to explain technical principles and does not replace Gaodun's finished product verification.
Further reading and technical information
The links below provide background on the topic. When it comes to specific performance, product selection or engineering parameters, please check the applicable objects and test conditions of each data.
- Covestro: Pasquick polyaspartic ester technical data (solutions.covestro.com)
- Asahi Kasei: Low viscosity and flexible design of polyaspartic polyurea flooring (asahi-kasei.co.jp)
The above original data is used to verify the corresponding technical principles, research formulas or construction examples, and is not the testing or certification of Gaodun products. Research conclusions should be understood together with formulas, specimens and test conditions; construction parameters of products from different manufacturers cannot be directly interchanged.