Polyaspartic Polyurea Technical ArticlesDesigning Wear Resistance in Polyaspartic Polyurea: Why Are Hardness, Scratch Resistance and Impact Resistance Not Interchangeable?
When polyaspartic polyurea is used for outdoor floors, clear topcoat and industrial surface protection, wear, scratches, impact and environmental aging need to be considered at the same time. Hardness is one of the indicators and cannot directly replace wear resistance. Gaodun combines open standards and 2025 network design research to discuss the impact of resin structure, particle dispersion, test conditions and system compatible system on surface durability. The surface protection performance of polyaspartic polyurea needs to be evaluated according to the actual damage pattern. Hard objects are pressed in, sharp objects are scratched, sand particles are repeatedly rubbed and falling objects impact, all of which have different stress processes.
Article contents (9 sections)
1. High hardness, why doesn’t it mean more durability under all wear conditions?
The surface protection performance of polyaspartic polyurea needs to be evaluated according to the actual damage pattern. Hard objects are pressed in, sharp objects are scratched, sand particles are repeatedly rubbed and falling objects impact, all of which have different stress processes.
| Performance | main concern | cannot be directly replaced |
|---|---|---|
| Indentation hardness | Resistance to local indentation | Cannot directly substitute for: Wear life and impact resistance |
| pencil hardness | Surface damage level under pencil action | Cannot directly substitute for: Scratch resistance under all contact conditions |
| Resistant to scratches | Damage caused by the specified stylus under the specified load | Cannot directly substitute for: Long-term repeated wear and tear |
| Wear resistance | Material loss or surface changes under specified friction conditions | Cannot directly substitute for: All actual wear conditions |
| Impact resistance | Cracking, denting and delamination under sudden loads | Cannot directly substitute for: Continuous wear performance |
Harder surfaces may resist some indentation or scoring, but actual wear also depends on toughness, crack development, friction conditions, and interfacial bonding.
Gaodun believes that the evaluation should start from "what damage will be suffered" and then select the corresponding indicators.
2. Different hardness methods cannot be directly converted into the same performance.
Shore hardness, pencil hardness and other surface hardness methods use different modes of action and evaluation scales. Results need to be stated together with method, temperature, curing time, thickness and substrate.
The pencil method of ISO 15184:2020 is suitable for smooth surfaces and can be used for relative grading of a group of coated panels with significant differences in hardness. When comparing across coatings, attention should be paid to the methodological limitations noted in the standard disclosure summary.ISO 15184:2020 Official Summary (iso.org)
Shore A, Shore D and pencil grades use different evaluation scales. For thick film or elastic systems, the thickness of the sample and the underlying support should also be checked to see if they affect the measurement. Scoring penetration can be evaluated in accordance with ISO 1518-1:2023 using a stylus with a specified load. If the drop weight causes rapid deformation, you can observe whether the dry film is cracking or peeling off the substrate according to ISO 6272-1:2011. These two methods respectively correspond to different injuries.
Gaodun advocates that hardness is used to track the state of the material under specified conditions; cross-formulation comparisons still need to be combined with actual damage testing.
3. The weight loss due to abrasion is small, so why do we need to look at the film thickness and surface changes?
ASTM D4060-25 evaluates organic coatings on flat, rigid substrates using a Taber abraser. A test report should identify the wheel, load, number of cycles, film thickness, curing conditions and how wear is reported. Gaodun report TL26080331 recorded a mass loss of 8 mg for the submitted specimen under GB/T 1768-2006, using a CS-10 abrasive wheel, a 750 g load and 500 revolutions (report page 3 of 6). When comparing, you should first check the test methods and conditions before judging whether the values are comparable. Gaodun test data and scope (gao-dun.com).
The standard specifically reminds that the condition of the grinding wheel, wear debris and filler may affect the comparison. Coatings containing higher density fillers may show greater mass loss but smaller thickness reduction.ASTM D4060 Official Summary (store.astm.org)
Therefore, when comparing formulas containing particles with those without particles, one cannot judge how much of the effective protective layer is consumed solely by the number of milligrams of weight loss.
Gaodun recommends common observations:
- Mass loss.
- Changes in wear scar depth or thickness.
- Whether the bottom is worn through.
- Surface morphology and particle shedding.
- Haze, gloss loss and visible scratches of the transparent layer.
Changes in the appearance of clear topcoat may appear before obvious wear and tear. For decorative protection, these changes also affect performance.
Data under different methods, grinding wheels or loads should retain their respective conditions and cannot be sorted directly.
4. Frontier Direction: Balancing Bearing and Energy Consumption through Network Collaboration
The public abstract of the 2025 paper in "European Polymer Journal" introduces the research on constructing aspartic acid ester-type urea-urethane coating using polypropylene carbonate diol, and reports the mechanical and friction and wear performance of the formula.Paper Source page (sciencedirect.com)
Mass loss during reciprocating wear testing was a reported wear result for the PPCDL-based research coating (DOI 10.1016/j.eurpolymj.2025.114100, abstract). For a Gaodun model, obtain that model’s wear test method, conditions and results. Mass loss alone does not establish a particular energy dissipation mechanism.
The specific results correspond to the research formula, reaction equivalent and wear conditions, and its optimal ratio or performance cannot be directly applied to other products.
Gaodun believes that collaborative research should be carried out around the prepolymer soft segment, resin structure, functionality and reaction ratio, and the performance after impact resistance, film formation and environmental effects should be checked at the same time.
5. The value of hard particles depends on the particles and resin working together.
Particles such as white fused alumina and silica can participate in surface wear-resistant design, but the actual effect is related to particle size, morphology, dispersion, addition amount, coating and particle-resin combination.
From the analysis of wear mechanism, if the particles are not stably fixed, they may fall off and become new abrasive particles; local agglomeration may also change leveling and surface defects.
Therefore, "harder particles" cannot alone be used to infer "the entire layer of coating is more wear-resistant". **
It should also be evaluated whether the particles remain bonded after repeated rubbing and water immersion.
For clear topcoat, it is necessary to coordinate the light scattering, haze and appearance changes caused by the particles; for anti-slip floors, it is necessary to evaluate the surface state after wear and wet anti-skid, and cannot judge based on the rough feel alone.
Gaodun advocates that the particle scheme should be verified together with the resin, film thickness and application structure, and the specific addition method shall be subject to the corresponding product process.
6. Outdoor wear resistance, you need to pay attention to the difference before and after environmental effects
Outdoor floors and industrial surfaces may first experience light, rain and temperature differences, and then undergo friction; wear and tear may also change subsequent water absorption, adhesion and media entry.
Gaodun proposed that two comparison paths can be set according to research goals:
| test path | Main observations |
|---|---|
| Aging first, then wear | Wear resistance after material state changes |
| Abrasion first, then water resistance or adhesion test | The impact of local damage on subsequent protection |
These are R&D design recommendations and are not automatically equivalent to a standard procedure.
Tests need to record temperature, moisture status, and age controls to avoid mistaking moisture or post-cure effects for permanent changes.
Good initial wear resistance is evidence; whether the target function is still retained after environmental effects requires further verification.
7. How should the combination of clear topcoat and decorative flake floors be evaluated?
Clear topcoat is responsible for appearance and surface protection, while decorative flake flooring also involves the connection of the bottom layer, decorative particles and topcoat. Each layer performing well alone does not mean the same stability when combined.
| Application | It is recommended to pay attention to |
|---|---|
| Transparent surface protection | Scratches, haze, gloss loss, yellowing and adhesion to the substrate |
| Decorative flake flooring | Abrasion, particle fixation, topcoat covering and interlayer bonding |
| outdoor traffic surface | Wet anti-slip, pollution, cleaning and changes after wear |
| Industrial equipment housing | Corrosion protection continuity at scratches, impacts and damage |
In the research on the compatible system of GaodunN600decorative flake floor and N200clear topcoat, the evaluation should be based on the corresponding structure, actual film thickness and curing conditions.
Material names or "high hardness" positioning are not substitutes for complete system results.
8. Gaodun’s technical stance: let surface indicators correspond to actual damage
Shenzhen Gaodun New Materials Co., Ltd. has focused on polyaspartic polyurea systems since 2016, focusing on the research and development, synthesis, formulation and production of Part A and Part B.
Gaodun believes that wear-resistant design should connect network structure, particle fixation, surface friction and interlayer bonding to match hardness, toughness and environmental stability.
For transparent protective layers, the appearance and adhesion should be maintained at the same time; for outdoor floors, attention should be paid to anti-slip and protective integrity after wear; for industrial surfaces, attention should be paid to whether mechanical damage weakens subsequent corrosion protection.
This article is a technical analysis and R&D evaluation suggestion. It does not mean that Gaodun has completed all the tests in this article. The hardness, wear resistance index, particle addition and compatible system requirements of specific models are subject to the corresponding technical instructions, test reports and construction processes.
Further reading and technical information
The links below provide background on the topic. When it comes to specific performance, product selection or engineering parameters, please check the applicable objects and test conditions of each data.
- ASTM D4060: Organic coating Taber wear and comparative limits (store.astm.org)
- ISO 1518-1:2023: Constant load needle scratch resistance test (iso.org)
- ISO 6272-1:2011: Main surface backlog head drop weight rapid deformation test (iso.org)
The above original data is used to verify the corresponding technical principles, research formulas or construction examples, and is not the testing or certification of Gaodun products. Research conclusions should be understood together with formulas, specimens and test conditions; construction parameters of products from different manufacturers cannot be directly interchanged.