Initial clarity describes the freshly applied finish. To assess clarity and gloss after aging, compare clarity, gloss and color before and after defined exposure using matched control panels with the same substrate and film thickness. This guide distinguishes whitening, gloss loss and yellowing and explains the role of an N200 site trial.

Article contents (9 sections)

1. What optical properties need to be controlled separately in the development of clear topcoat?

When transparent coatings are used on decorative flake floors, wood, stone and composite materials, they must provide protection while retaining the texture and color of the substrate.

"Looking transparent" doesn't fully describe this ability. BYK's optical evaluation data divides transparency performance into aspects such as total light transmittance, haze and clarity. BYK: Transparency Measurement Technical Description (byk-instruments.com)。

For transparent polyaspartic polyurea, you should also pay attention to:

Table 1
Properties Main content Possible appearance changes
Translucent performance Can light pass through materials? Overall darkening and reduced light transmittance
Haze and clarity To what extent is light scattered after passing through it? Foggy, blurred textures
color selective absorption of visible light Turns yellowish initially or yellowing after use
surface gloss The reflective state of light on a surface gloss loss, scratches, roughening

A coating may have high light transmittance, but the texture cannot be seen clearly due to scattering; it may also be very clear, but with a yellowish tint.

Therefore, Gaodun believes that clear topcoat should establish a multi-index evaluation to avoid summarizing all performance with a single "high transparency".

2. The original solution is clear, why may it still become foggy after curing?

Part A and Part B are respectively clear, which does not prove that they are always compatible throughout the mixing and curing process.

When a two-part clear finish turns cloudy, record the appearance of the mixture, the freshly applied wet film and the cured film. Keep the substrate and applied film thickness consistent across panels. Identify when cloudiness first appears. Attributing it to microscopic phase separation during cure requires structural evidence.

A loss of clarity may become visible when differences in the size or refractive index of these regions cause sufficient light scattering. Microscopic inhomogeneity does not necessarily mean that it is white to the naked eye, and whether microphase separation has occurred cannot be judged based on appearance alone.

BYK's transparent film technical information explains that pores, crystals and other inhomogeneous structures within the material, as well as surface structures, may cause scattering. Applying this optical principle to the research and development of polyaspartic polyurea needs to be combined with specific formula verification. BYK: Transparency Measurement Technical Description (byk-instruments.com)。

Gaodun focuses on compatibility throughout the entire process of storage, mixing, curing and aging. Just looking at whether it is clear when first mixed, the evidence is still insufficient.

3. How do microbubbles and additives affect transparent performance?

There are clear optical differences between the inside of the bubbles and the resin. A large number of small bubbles may make the transparent coating appear milky even if it is difficult to identify them one by one.

When investigating bubbles, record whether they first appeared in the mixture, after application or during cure. Page 4 of the Simplified Chinese Gaodun N200 TDS calls for minimizing air entrainment during mixing and applying a uniform thin coat. A photograph of the cured bubbles cannot identify the gas source.

Therefore, transparent systems need to coordinate initial viscosity, wetting, foam removal and cure speed.

Defoaming agents, leveling agents and wear-resistant components also need to be evaluated for compatibility. Just because a certain additive performs well in paint does not mean that it will still have the same appearance after being used in clear topcoat.

When inorganic particles are introduced, transparency cannot be judged only at the "nano level". Particle size distribution, degree of agglomeration, refractive index differences and additive amounts all affect scattering.

Gaodun believes that wear resistance enhancement and transparency maintenance should be evaluated simultaneously to avoid sacrificing texture presentation in order to improve a certain indicator.

4. If it turns white when exposed to water, does it mean that the resin has been hydrolyzed?

For a clear finish that whitens on contact with water, record the substrate, contact time, wet appearance and appearance after drying under defined conditions. Compare it with a matched panel kept dry. Diagnosing hydrolysis requires chemical evidence beyond a photograph of whitening.

In research and development, we first need to distinguish: can it be restored after drying? How long does recovery take? Are there cumulative changes after repeated wetting and drying? Do adhesion and mechanical properties decrease simultaneously?

If it returns to transparency after drying, it means that the appearance change is reversible to a certain extent, but other performance changes cannot be ruled out based on this. If whitening continues or is accompanied by blistering, further analysis of the film body and interface is required.

Hydrolysis is a change in chemical structure and should be judged in conjunction with appropriate chemical analysis and performance evidence.

For clear topcoat, Gaodun advocates recording the "wet appearance" and "restored appearance" at the same time, and then combining the adhesion, blistering and other results to establish a complete judgment.

5. What is the difference between yellowing and whitening of transparent materials?

Record yellowing, haze and gloss separately. For planar, light-transmitting specimens within its scope, ASTM D1003 measures haze and luminous transmittance. Use a suitable color method for yellowness. Check material, thickness and appearance when comparing yellowness indices. A coating on an opaque project substrate cannot serve as a transmission specimen.

The color stability of transparent polyaspartic polyurea needs to examine the overall structure of Part A and Part B, the initial color of raw materials, residues, additives, and photothermal oxidation changes during use.

For N200 on a specific substrate, assess clarity and gloss retention using comparative records for that grade, substrate and system under the intended exposure. Page 4 of the Simplified Chinese N200 TDS calls for a trial of clarity, color, adhesion and intercoat compatibility before application. That trial provides a baseline. Long-term color retention requires follow-up exposure records.

Thickness also affects color observation. Thicker specimens may be more susceptible to subtle tints, so film thickness, background, and measurement conditions should be controlled when comparing different formulations.

For transparent products, "low initial chroma" and "little color change after aging" should be stated separately as two indicators.

6. Transparent coating is stable by itself, so why might it still fail to protect the substrate?

Clear topcoat needs to allow visible light to pass through, but this does not mean that it can fully block ultraviolet radiation that causes changes in the substrate.

To assess appearance retention, compare clarity, gloss and color before and after exposure. Prepare matched coated panels with the same substrate and film thickness, and record exposure conditions and duration. Keep an uncoated sample of the same substrate to check for substrate discoloration. An installation photo records only the initial appearance.

BASF public information divides light stabilization technology into different paths such as absorbing ultraviolet radiation and inhibiting degradation caused by free radicals. BASF: Light Stabilizers Technical Note (dispersions-resins.basf.com)。

There is a difference in the functions of UV absorbers and hindered amine light stabilizers. Formula design needs to take into account the absorption band, compatibility, film thickness and usage environment. The effect cannot be judged solely by the amount added.

The weather resistance of transparent coating itself and its ability to protect the substrate need to be verified separately.

This is also an important reason why clear topcoat research and development has moved from single film evaluation to actual coating system evaluation.

7. How to create a convincing clear topcoat evaluation?

Gaodun believes that at least standardized samples and actual substrate combinations need to be observed simultaneously.

Standardized samples are useful for comparing changes in color, haze and light transmission of resin formulations; actual decorative flakes, wood or stone test panels are used to evaluate texture presentation, interface and overall appearance.

The public summary of ISO 14782:2021 limits the haze method to clear, essentially colorless plastics with less than 40% haze, and cautions that worn or frosted surfaces may give lower readings. ASTM D1003-21 specifies the haze and light transmittance ratio measurement method for flat transparent plastics. When comparing transparent coating films, the sample preparation, film thickness and measurement method should be recorded, and the same method should be used to compare before and after aging. When topcoat is attached to opaque ceramic tiles, stone or wood, a compatible systems site test is also used to evaluate the reflective appearance, color difference and gloss.

Table 2
Evaluation stage Suggested observation items critical control conditions
After initial cure Color, haze, gloss, bubbles and texture clarity film thickness, curing time, background
After immersion and recovery Degree of whitening, recovery, blistering and adhesion Water temperature, time, recovery conditions
After photoaging Changes in color, gloss, haze and cracks Light source, circulation, sample temperature
After wear Scratches, gloss loss and texture visibility Wear patterns, loads and cleaning methods
After outdoor exposure Changes in the combination of coating, substrate and interface Orientation, climate, maintenance and records

The above content belongs to the R&D evaluation path, and specific product conclusions should be supported by the corresponding model, substrate and testing conditions.

8. Gaodun’s R&D direction: Make transparent protection verifiable after use

The engineering value of clear topcoat is reflected in whether it can retain the appearance of the substrate after use and continue to play a protective role.

Towards this goal, Gaodun focuses on the synergy between the compatibility of Part A and Part B after reaction, micro-bubbles control, water-resistant appearance maintenance, light stabilization system and substrate adaptation.

For decorative flake floors, both texture clarity and wear resistance need to be taken into consideration; for wood, it is necessary to pay attention to the discoloration and dimensional changes of the substrate; for stone and composite materials, it is necessary to combine the interface and overall appearance evaluation.

When adding hard segments, wear-resistant particles or light-stabilizing components, changes in transparency, flexibility and adhesion should be checked simultaneously.

Gaodun's technical judgment on transparent polyaspartic polyurea is: initial clarity provides a starting point, and it can still maintain applicable optical and protective properties after experiencing water, light and abrasion, so that it can reflect long-term use value.

Further reading and technical information

The links below provide background on the topic. When it comes to specific performance, product selection or engineering parameters, please check the applicable objects and test conditions of each data.

The above original data is used to verify the corresponding technical principles, research formulas or construction examples, and is not the testing or certification of Gaodun products. Research conclusions should be understood together with formulas, specimens and test conditions; construction parameters of products from different manufacturers cannot be directly interchanged.