POLYASPARTIC TECHNICAL ARTICLES

Polyaspartic Polyurea Technical Articles

Designing Chemical Resistance in Polyaspartic Polyurea: From Swelling Mechanisms to Practical Protection Limits

Specify the chemical, concentration, contact temperature, duration and exposure mode before selecting a coating. Check data for the proposed grade and system. This article distinguishes changes in appearance, mass, dimensions and adhesion, and explains the separate saltwater immersion and abrasion results in report TL26080331.

Article contents (9 sections)

1. Resistant to chemical media, why do we need to specify the specific conditions?

Although the floor comes into contact with cleaning agents, industrial equipment comes into contact with oil, and the roof encounters pollutants, although they all involve chemical media, the contact methods and failure mechanisms are different.

The fact that the appearance of a material does not change in a certain dilute acid for a short period of time does not prove that it is suitable for high temperature, concentrated acid or long-term immersion. Water resistance is good, and resistance to organic solvents cannot be directly derived.

ISO 2812-1:2017 provides methods for evaluating the resistance of single or multi-layer coatings to the effects of liquids other than water and involves the evaluation of damage to the substrate when necessary.

Gaodun believes that a verifiable technical statement should at least answer: what medium, what concentration, what temperature, how long the contact is, what method is used, and what indicators are used to judge.

"Acid and alkali resistance" should correspond to a clear set of results to support specific selection.

2. What changes may occur after the medium enters coating?

The interaction between chemical media and coating can involve physical processes or chemical reactions, and both may exist at the same time.

Table 1
process Possible changes What needs further confirmation
Absorbing and sleeping Increase in mass or volume, softening Can it be restored after being separated from the media?
Plasticization Decreased modulus, increased indentation or deformation Whether it still meets the requirements under the operating load
extraction If mass decreases after drying, identifying what was extracted requires separate evidence Changes in mass, appearance and properties after drying
chemical structural changes hydrolysis, oxidation or other reactions Is there chemical analysis and evidence of performance?
Interface degradation Record blister locations and the failure plane in the adhesion test before attributing damage to an interface Is the damage located within the membrane, between layers, or at the substrate interface?

"Undissolved" does not mean that properties remain unchanged. Even if the cross-linked coating film maintains its overall shape, it may absorb the medium and undergo significant swelling.

There is no change in appearance, and it cannot alone prove that the adhesion and mechanical properties still meet the requirements.

3. Why does increasing the degree of cross-linking not guarantee that all media resistance indicators will increase at the same time?

For a swelling assessment, identify whether the specimen is a free film or a coating on a substrate. Record measurements before immersion, after removal and after drying under defined conditions. Compare mass or dimensional changes at the same liquid composition, concentration, temperature and immersion time.

Therefore, the degree of cross-linking and the chemical structure of the segments need to be analyzed together.

To assess chemical resistance, specify the chemical, concentration, contact temperature, duration and type of exposure: occasional splashes, repeated contact or continuous immersion. Check test records for the proposed finished coating and system under those conditions. Raw-material functionality or hard-segment content alone gives no acceptance result for that exposure.

For Gaodun's Part A and Part B collaborative design, it is necessary to simultaneously examine reaction equivalent, effective conversion, soft and hard segment structure, and network uniformity.

Deviating from the prescribed ratio and adding a certain component cannot be used as a general method to improve chemical resistance. Inadequately reacted components and network defects may alter absorption and extraction behavior.

R&D should pursue a network structure suitable for the target medium and verify its performance balance.

4. Acid resistance, alkali resistance and solvent resistance, why can’t they be replaced by each other?

In polyaspartic polyurea there are urea bonds, ester groups, and other segments depending on the design of Part A. The responses of these structures to different media are not the same.

For aqueous solutions of acids and alkalis, attention needs to be paid to concentration, temperature, contact time, and the structures in the formula that may be affected. Under sufficiently severe conditions, ester groups may participate in the hydrolysis reaction; however, the actual alkali resistance level of a product cannot be determined solely by the presence of ester groups.

For organic solvents, swelling, plasticization, and extraction may be more straightforward than short-term chemical bond breaking. Alcohols, ketones, esters and hydrocarbons cannot be treated as the same medium.

Actual oils and cleaners are often mixtures and may contain additives, surfactants or other ingredients. Testing only one base oil or single solvent may not be representative of the actual formulated liquid.

Gaodun advocates that after basic screening, further verification should be carried out using the actual media specified by the project. Just because the pH is the same is not enough to determine that the two solutions have the same effect on coating.

5. How to distinguish between short-term dripping and long-term soaking?

Timely cleaning after splashing, repeated scrubbing, local accumulation of liquid and continuous soaking put different requirements on materials.

FLEXMAR’s chemical resistance chart covers two coatings, Self-Prime HS and Clear Coat HS, for chemical splash-and-spill exposure. Continuous immersion requires test evidence for the specific coating, chemical and exposure duration. View the FLEXMAR chemical resistance chart (flexmarpolyaspartics.com)

ASTM D543-21 also points out that the correlation between the test and actual use depends on the degree of similarity of conditions; for continuous immersion applications, short-term tests mainly provide screening significance. This standard is oriented to plastics, and applicable methods should still be selected for specific coating projects. ASTM D543-21 Official Summary (store.astm.org)。

Gaodun believes that the short-term contact test is suitable to answer "can it be cleaned and recovered after occasional contamination", while continuous immersion needs to answer "can the medium maintain protection after long-term action".

The two results can complement each other, but are not direct substitutes.

6. Why can a small change in mass mask damage?

When evaluating swelling, it is often necessary to compare the mass of the specimen before and after contact with the medium:

Mass change rate = (mass after exposure - initial mass) ÷ initial mass × 100%.

To use this indicator, the wiping method and weighing time after sampling must be specified.

The sample may absorb the medium and lose extractable components at the same time. When the two processes are partially offset, the net mass change is small and may still be accompanied by structural and performance changes.

Therefore, the state after exposure and the state after drying can be recorded separately under specified conditions, and combined with analysis of dimensional, hardness, tensile or adhesion changes.

ASTM D543-21 involves reports on changes in mass, dimensions, appearance and mechanical properties. For polyaspartic polyurea research and development, the combination of multiple indicators helps avoid single-point judgment. ASTM D543-21 Official Summary (store.astm.org)。

At the same time, the free film and the actual coated test plate should be evaluated separately: the former is conducive to observing the material body, and the latter can incorporate the influence of substrate and interface.

7. From a single immersion test to the evaluation of the interaction between medium and load

Actual floors may withstand vehicle steering when contaminated by oil; equipment coatings may experience temperature differences when exposed to cleaning agents; outdoor coatings may age first and then be exposed to chemical media.

If abrasion follows immersion in service, document the test sequence, whether the specimen was wet or dry during abrasion, and the applied load. Separate immersion and abrasion tests establish only the results recorded for each test.

Report TL26080331 lists abrasion and saltwater resistance separately. The submitted specimen underwent 1,000 hours of immersion in 3% NaCl solution. This was a saltwater immersion test; the report gives neither a salt spray result for that exposure nor a wet-abrasion result after immersion. It lists no separate values by product grade. For a specified grade, obtain records for its coating system and intended exposure.

The research and development direction Gaodun focuses on is to introduce well-founded combination conditions based on applications:

Table 2
Application conditions Possible verification directions
Oil pollution and traffic Hardness, wear and adhesion after exposure
Periodic cleaning Actual cleaners, scrub cycles and recovery
Outdoor industrial protection Comparison of media resistance and adhesion before and after aging
long-term local effusion Continuous contact, blistering and interface changes
Deformation or temperature difference environment Combination of media with controlled strain and temperature cycling

The combined evaluation should be set around known usage conditions, and control samples should be retained to facilitate judgment of the role of each factor.

8. How does Gaodun create media-resistant data that can be used for model selection?

Gaodun believes that media resistance data should allow customers to understand the applicable scope and trace it back to the corresponding products and samples.

Each result should include product model, ratio, film thickness, substrate, curing conditions, medium information, exposure conditions, recovery conditions and judgment indicators.

For clear topcoat, attention should be paid to color difference, gloss loss, whitening and adhesion; for industrial protection, attention should be paid to continuity, blistering and substrate status; for floors, it is also necessary to combine the load-bearing and wear-resistant performance after exposure.

These contents belong to the direction of R&D and technical data construction and cannot replace the test results of specific models.

For long-term research and development, Gaodun focuses on improving the performance retention capability under target medium conditions through raw materials structure, solidification network and interface design, and uses corresponding experiments to determine the boundaries.

The chemical resistance value of polyaspartic polyurea should be reflected in: under specific media and use conditions, the coating can still maintain the required appearance, mechanical and protective properties.

Further reading and technical information

The links below provide background on the topic. When it comes to specific performance, product selection or engineering parameters, please check the applicable objects and test conditions of each data.

The above original data is used to verify the corresponding technical principles, research formulas or construction examples, and is not the testing or certification of Gaodun products. Research conclusions should be understood together with formulas, specimens and test conditions; construction parameters of products from different manufacturers cannot be directly interchanged.